Quality control of gray cast iron melt
Pig iron is one of the main raw materials of gray cast iron. Figure (a) shows the metallography of pig […]
Pig iron is one of the main raw materials of gray cast iron. Figure (a) shows the metallography of pig […]
The casting die is made by lost foam casting, and the foam model is combined with the model. The foam
Gray cast iron is one of the most commonly used metal materials for automotive parts such as engine, because of
High quality and high strength gray cast iron should have fine and uniform A-type graphite and fine flake pearlite matrix
Cast steel joints are widely used in airport terminals, railway stations, stadiums and other large public buildings because of their
As the largest automobile production and consumption country in the world, China has huge development space and broad prospects for
As an excellent wear-resistant material, high manganese steel is often used in metallurgy, mining, cement and other industries, such as
The influence of alloying elements on the microstructure of cast iron mainly occurs in two stages: solidification stage, in which
Gray cast iron is often used to manufacture engine block and other smart car parts because of its unique properties.
Lost foam casting nodular cast iron has the advantages of good surface quality, high dimensional accuracy and high process yield.
With the rapid development of industrial technology, people have higher and higher requirements for material properties, as well as gray
1. Determination of initial and boundary conditions for numerical simulation of turbine rear exhaust nozzle casting The results show that
The microstructure and properties of high strength gray cast iron produced by sand casting were improved; The effect of hard
Cast iron generally refers to a multi-component iron carbon alloy with a C content of more than 2.0% (wt%, the
Iron castings are widely used in various mechanical equipment, construction, metallurgy, agricultural machinery, national defense industry and other fields. In
The research object comes from the turbine rear exhaust pipe of ZHY casting. The turbine rear exhaust pipe is the
ANSYS is a general-purpose finite element software that can adapt to the coupling analysis of a variety of physical fields.
The dual liquid bimetallic lining plate is a technology for preparing new composite wet wear resistant metal materials by using
The vibration lost foam casting technology is to apply a certain frequency and amplitude of mechanical vibration in the lost
This paper mainly studies the effects of quenching temperature of destabilization treatment and natural aging treatment on the microstructure and
It can be seen from the discussion results that when the metal solidifies, the vibration will increase the undercooling of
The defects of traditional casting composite interface are avoided in principle. Solve the following problems: 1). Ordinary white cast iron,
The vibration solidification technology of lost foam casting is a physical modification technology to refine the grain size and improve
The effects of destabilizing heat treatment temperature and natural aging treatment on the microstructure and properties of high chromium cast
The graphite in gray cast iron is flake, which is the most widely used cast iron, and its output accounts
The research object is high chromium cast iron carbon steel bimetallic wear-resistant liner. Its quality mainly depends on whether the
In the practical application of lost foam casting in China and abroad, the lost foam casting of cast iron alloy
Aging refers to the heat treatment process when the tempering temperature is lower than 100 ℃. The newly formed martensite
The control of the composite interface focuses on two aspects: one is to ensure the flatness of the composite interface,
The bimetallic jaw wear-resistant castings were successfully poured by using bimetallic liquid pouring / transformation molding technology. The composite casting