Development characteristics of lost foam casting technology in China
The development of lost foam casting technology in China has the following characteristics: 1) Township enterprises and small and medium-sized […]
The development of lost foam casting technology in China has the following characteristics: 1) Township enterprises and small and medium-sized […]
1. Manufacturing process All the technologies described above have different advantages. In this study, selective laser sintering technology is mainly
Additive manufacturing technology includes computer-aided design technology, material processing and forming technology. At the same time, digital model files need
In addition to composite rollers and composite pipes, ring parts such as bearing rings and flanges are used as key
A lot of research and application have been carried out on Squeeze Casting Technology in foreign countries. For example, casting
The bimetallic jaw wear-resistant castings were successfully poured by using bimetallic liquid pouring / transformation molding technology. The composite casting
The physical and mechanical properties of bimetallic composites are different. Although the two metals maintain their original characteristics, their comprehensive
China has also carried out numerical simulation of casting solidification since 1978. Although it started late, it has also developed
Since the 1960s, forsund, Denmark, first applied the finite difference method to study the numerical simulation of solidification process, which
The basic idea of computer solidification simulation is that firstly, the geometric modeling of casting entity is meshed and discretized
The level of numerical simulation has reached a high level in developed countries, especially in the United States and Europe
Compared with foreign countries, the research on numerical modeling of casting solidification in China started late, but made rapid progress.
The basis of casting process design is the casting forming theory. The casting forming theory studies the mechanical, physical and
Firstly, cast the steel castings of the coupler according to the original casting process design. The main problems exposed are:
Due to the differences in product structure, weight, process equipment of production enterprises, production conditions and process technology level, there
For thousands of years, people have mainly solved engineering problems through trial and error, especially how to produce high-quality castings.
As a material processing technology that has been used for thousands of years, sand casting is the most direct way
1. Molding operation process In the original process (see Figure), the type is divided from one end, and the gray
At present, the production of heavy-duty lathe locking block has the advantages of low yield, high cost, complex on-site operation
Excavators are widely used in mining, civil engineering, water conservancy and national defense projects. Bucket teeth are not only important
The casting material brand of brake drum is HT250, which adopts Yingda electric furnace to melt molten iron, fcmx Xindong
Al-Si alloy has good casting properties. After modification, inoculation and heat treatment, it has good comprehensive mechanical properties, corrosion resistance
Aiming at the research and application of preparation technology of high-performance nodular cast iron crankshaft, an exploratory study was made
In CATIA three-dimensional modeling software, save the component digital models of sand casting and gating system as STL format and
The casting process of crankshaft affects the quality of crankshaft. The casting process parameters include sparing injection temperature, winding injection
With the rapid development of automobile industry, the production and sales of engine are also increasing year by year. As
Comparing the cooling curves of sand mold, iron mold sand coated casting and metal mold casting, it can be seen
The engine is known as the “heart” of the automobile, and the cylinder head is one of the most important,
1. Floating core There are regular pits on the upper surface of nodular cast iron. After dissecting the nodular cast
The casting adopts the green sand production process, and the sand core is made of coated sand. The mold plate