Types of spent fuel storage and transportation vessels and advantages of ductile iron vessels
The metal container for dry storage is the key equipment for the transportation and storage of spent fuel, and it
The metal container for dry storage is the key equipment for the transportation and storage of spent fuel, and it
Germany has realized the mass production of 100 ton nodular iron nuclear spent fuel containers, and has produced more than
Based on the simulation analysis of the casting process of 100 ton ductile iron nuclear spent fuel container, the 45
In order to eliminate the adverse effect of hot spot, reduce the defects of ductile iron spent fuel container and
The simulated solidification time distribution of ductile iron spent fuel container is shown in the figure. As can be seen
The thickness of chill is designed according to the chill of gray iron casting, as shown in the formula Where
The service conditions of ductile iron nuclear spent fuel container are harsh, the performance requirements are strict, especially the low
The as cast microstructure and properties of lzqt600-3 ductile iron profile were studied. Firstly, according to GB / T 9441-2009
As shown in the figure is the structure diagram of polished state of lzqt600-3 ductile iron section edge, 1 /
Tensile test Ht-2402-100kn universal testing machine is used to measure the tensile properties of ADI in strict accordance with GB
Temperature test of molten iron Ya1-w330 portable melting thermometer is used to measure the molten iron temperature in the process
After the ductile iron test bar is taken out of the box, the angle grinder is used to cut the
Ordinary clay sand molding is adopted, and the molding process includes mold processing, sand mixing, sand pounding, box turning, vent
The spheroidizing treatment was carried out by the method of in package charging. The spheroidizing temperature is 1450 ~ 1500
When the chemical composition of molten iron is constant, the smaller the casting modulus, the higher the amount of P
When the high temperature molten iron is poured into the furan resin self hardening sand mold, the furan resin, curing
The design of sand core head of intake cylinder is the most important content in sand core design, and also
Visual observation of the test block section with a thickness of 400mm shows that there are dense distribution of suspected
In order to study the effect of composition on the morphology of thick and large section graphite, bulk sampling was
The chemical composition directly affects the matrix structure and mechanical properties of nodular cast iron castings. Reasonable chemical composition is
When the carbon content is increased to solve the shrinkage cavity and porosity defect, the top graphite floating and the
① According to the ratio of cross-sectional area, it is divided into closed gating system and open gating system. The
① The main function of the sprue is to guide molten iron into the runner or runner. According to the
Features: the fracture surface of the casting is gray black, and the mechanical properties are obviously low. Through metallographic examination,
Graphite floating means that there are a large number of graphite balls on the upper surface of the casting, and
There are three types of slag addition: the first type of coarse slag is 2mg · SiO2 + MGS or
Asphalt paint coating Asphalt paint coating is used to transport gas pipeline. Preheating the pipe before painting can improve the
As we all know, the quality of nodular cast iron is related to the material and technology used. Besides, the
Ductile iron have almost been applied in many main industrial sectors, where high strength, good plasticity, excellent toughness and wear