Casting process of nodular cast iron piston ring of Japan piston ring company (NPR)
NPR’s foundry is located in Iwate, Sendai City, 250km away from Tokyo, in Northeast Japan. It was built in 194.
NPR’s foundry is located in Iwate, Sendai City, 250km away from Tokyo, in Northeast Japan. It was built in 194.
The company is one of the oldest Piston Ring Companies in the world, with a history of more than 120
The lost foam casting process of nodular cast iron was studied by using ProCAST software and visual environment software. The
The lost foam casting Pouring Scheme of ductile iron mainly includes pattern making, layout of ductile iron castings, design of
1. Nodular cast iron molding process The two box core molding is adopted to enlarge the sand filling core of
Nodular cast iron intercooler base pipe is an innovative design for the company’s large internal combustion engine. The material is
According to the characteristics of Si Mn alloyed ductile iron grinding ball, the heat treatment equipment should have the characteristics
To do a good job of Si-Mn alloyed nodular cast iron grinding ball, first of all, spheroidize the nodular cast
The above improvement scheme is used to verify the pouring production. Figure 1 is the foam pattern cluster and the
According to the trial production and simulation results of the two schemes of bottom injection and top injection, the bottom
The systematic study of wear-resistant materials has a history of more than 100 years. Different types of wear-resistant materials, such
Comprehensively considering the solidification simulation results and trial production results of the two trial production processes of nodular cast iron
Figure 1 a) ~ C) shows the top injection solidification process. In step 620, it can be seen that the
The casting process design and casting process of high strength and Toughness Nodular Cast Iron for automobile hub support were
Starting from the practical application of sand casting production process, the process design and material properties of nodular cast iron
The casting process of hub support is simulated and calculated by using magma simulation software, the shortcomings of the original
The powerful surface function of UG is used to carry out three-dimensional modeling of complex long forks. The feature modeling
There are two main classification methods of gating system: one is divided into closed type, semi closed type and open
The selection of chemical composition should be considered from two aspects: ensuring good mechanical properties and casting properties of castings.
In order to obtain nodular cast iron that meets the requirements of high strength and toughness of automobile hub support,
Hub support is an important supporting component of automobile suspension system. During automobile driving, it mainly bears alternating impact load,
The tensile properties of nodular cast iron are mainly related to the quantity and quality of graphite balls and the
1.Mechanical property 1) Tensile strength As the most common stress state, tensile stress is closely related to other static load
In the process of cooling to room temperature, the microstructure of nodular cast iron may follow two paths of phase
As a widely used metal material, cast iron has a long history of development. China is one of the first
According to the comparison of the numerical simulation results of the scheme, it is found that by reasonably increasing the
It can be found from the analysis that simply changing the height of the pouring riser of nodular cast iron
Firstly, from the aspect of changing the height of nodular cast iron pouring riser, without changing the diameter and neck
According to the simulation results in the previous section, it is found that the feeding channel of riser neck is
The temperature distribution of nodular cast iron during solidification of automobile hub support is shown in Figure 1. As can