Simulation results of filling process of nodular cast iron for hub support
Nodular cast iron belongs to a typical paste solidification mode. The possibility of shrinkage porosity, shrinkage cavity, air hole, slag
Nodular cast iron belongs to a typical paste solidification mode. The possibility of shrinkage porosity, shrinkage cavity, air hole, slag
(1) Material definition The material used in the simulated automobile hub support is the high strength and Toughness Nodular Cast
Using ugnx12 0 software to model the pouring and feeding system of automobile hub support. UG NX12. 0 is a
After the molten metal is poured into the mold, it usually produces volume shrinkage in the process of solidification and
After determining the type and layout of the nodular cast iron gating system, it is necessary to calculate the specific
The function of sand core is to shape the hole, inner cavity or parts that are not easy to produce
To design the process of nodular cast iron, in addition to selecting the correct casting method and process scheme, the
The selection of parting surface is directly related to the dimensional accuracy, production cost and efficiency of nodular cast iron.
According to the actual production situation, the automobile hub support casting is produced by using the Japanese Xindong automatic pouring
Spheroidizing treatment and inoculation treatment are essential pre furnace treatment steps for raw molten iron of nodular cast iron. The
In order to obtain as cast ferrite pearlite nodular cast iron with high strength and good plastic toughness, the production
The automobile hub support is an important support of the rear suspension system of the car, one for the left
The metallographic samples of nodular cast iron No. 1 ~ 3 nodular cast iron corroded by 4% nitric acid alcohol
(1) Sample preparation. Cut the samples of three components into 10 mm by wire cutting machine × 10 mm ×
Nodular cast iron intercooler base pipe is an innovative design for the company’s large internal combustion engine. The material is
1. Chemical composition design When the diameter of roll body is more than 600 mm, the carbon equivalent is 3.8%
1. Main quality problems of rolls Produced φ 800 mm × 1880 mm high chromium cast iron roll (as shown
The medium frequency furnace is used to produce cast iron rolls of various purposes and materials, and the core is
In the 1980s, Siempelkamp company of Germany successfully developed castor series nodular cast iron transport containers. Compared with other metal
1. Metallographic comparison The metallographic structure comparison before and after the improvement of the process of producing nodular cast iron
1. Molding process The two box core molding is adopted, and the sand filling core under the side molding is
1. Spheroidizing treatment Graphite distortion and fragment graphite will be produced in nodular cast iron with thick and large section
The solidification characteristics of heavy section nodular cast iron castings are: short liquid solidification time, long eutectic solidification time, and
The shell of the water ring vacuum pump used by ZHY Casting is welded with steel plates and processed into
Table 1 shows the impact absorption energy of nodular cast iron V-notch samples at different ambient temperatures. The samples are
1. Advantages Referring to the Research Report of zhangboming et al. And in combination with the analysis and research of
1. Chemical composition detection Arl3460 direct reading spectrometer is used for chemical composition detection, and the chemical composition detection results
1. Molding sand properties In order to ensure good surface quality of castings, the performance of green molding clay sand
1. Layout design Disa230b vertical parting boxless injection molding machine is adopted, and the size of molding machine plate is
With the rapid development of the automotive industry, the requirements for automotive castings are getting higher and higher, and the