Heat treatment technology in the production of China large steel castings
After pouring of large steel castings, there are great differences in the cooling rates of different parts, appearance and core
After pouring of large steel castings, there are great differences in the cooling rates of different parts, appearance and core
Large castings have long production cycle and complex processes. Generally, they have to go through many processes. Reasonable setting of
Large steel castings in the fields of nuclear power, hydropower, thermal power and metallurgical equipment have strict service conditions and
Compared with industrial developed countries, there is a big gap in the production of large steel castings in China in
There are more than 30 large-scale casting production enterprises in China, most of which are large and medium-sized state-owned enterprises.
1.With the expansion and transformation of some steel casting industries and the large investment and construction of local private enterprises,
1.Mainstream enterprises refer to some former national enterprises, which make use of the advantages of equipment conditions and further carry
1. Talent training and platform construction The development of the industry is inseparable from the support of professional talents, especially
Although China is a large foundry country, it is not yet a powerful foundry country. Compared with industrial developed countries,
The strength, especially plasticity and toughness of steel casting parts are greatly reduced due to coarse grains, uneven microstructure and
The strength, especially plasticity and toughness of steel castings are greatly reduced due to coarse grains, uneven microstructure and internal
Casting process is a process scheme to ensure that steel casting parts have complete shape, clear outline and no internal
Modification and microalloying is one of the hotspots to improve the properties of steel casting parts for many years. Through
As we all know, the performance of steel casting parts comes from casting materials, guaranteed by manufacturing process and improved
The foundry has formulated the quality control inspection process according to the casting process. The owner, the general contractor and
The chilling effect of the cold iron will change the local cooling rate of the steel casting, so that the
After analyzing the hot spot position and feeding channel of steel castings, the position of riser can be determined. In
Generally speaking, the riser should be set at the hot joint of steel castings, that is, the final solidification area.
During solidification, the steel casting will produce liquid shrinkage and solidification shrinkage. When the feeding system cannot provide sufficient liquid
According to the analysis of the original process scheme of the valve body, it can be seen that the improper
In order to ensure that there is no dead corner in the negative pressure inside the sand box, 5 air
Lost foam casting is a negative pressure full mold casting technology developed on the basis of vacuum sealing molding combined
According to the gear specification, the design structure of cast steel gear is divided into full circle structure, 1 /
Large steel castings are mostly the main bearing parts and supports in major technical equipment. The castings have huge size,
The manufacturing industry of large steel castings is the basic industry of national equipment manufacturing, and its development level is
China’s steel casting parts are indispensable products for China’s equipment manufacturing, the basis of national equipment manufacturing, and occupy a
China steel casting parts manufacturing industry is the basic industry of national equipment manufacturing, especially the manufacturing of large China
There are more than 30 large-scale casting production enterprises in China, most of which are large and medium-sized state-owned enterprises.
In the late 1920s, Robertson first discovered the medium temperature transformation product later named bainite in steel. Later, the researchers
The tempering process is the quenching and tempering step after the previous heat treatment. Although the martensite in the structure