Wear resistance mechanism of cast steel liner of cone crusher
Combined with the performance requirements and development direction of crusher lining material, a new bainite Martian multiphase wear-resistant cast steel
Combined with the performance requirements and development direction of crusher lining material, a new bainite Martian multiphase wear-resistant cast steel
As a big foundry country, the development level of China’s foundry industry is constantly improving. However, the problem of casting
The typical specification characteristics of section steel universal edging roll and special-shaped steel s-roll products are that the roll neck
Riser is a kind of structure for storing liquid metal in the mold, which is used to compensate the possible
Through the observation of the defects, it is found that the defects are shrinkage porosity and shrinkage cavity, which are
Metal bending test is a test method to measure the bending plastic deformation ability of metal materials under bending load,
The working conditions of hydraulic turbine equipment are strict, and runner, as the core component of hydraulic turbine, has been
Scheme 1 According to the simulation results in Fig. 1 (E), the whole filling process takes about 19.6 s, which
The gating system is the channel in the sand mold to guide the molten steel into the cavity. In the
The working conditions of hydraulic turbine equipment are strict, and runner, as the core component of hydraulic turbine, has been
Traditional measurement methods include manual measurement and large-scale three-dimensional scribing instrument, which have low measurement accuracy, high error rate, low
At present, the dimension measurement methods commonly used in large steel castings are traditional manual measurement, three-dimensional scriber and so
(1) Reduce the level of non-metallic inclusions in castings. The main purpose is to improve the purity of liquid steel.
The structure of the water-cooled steel brick casting is complex (see Figure), and the water pressure test of 0.5MPa is
ZG35CrMo material has poor casting performance, high solidification shrinkage and easy to produce shrinkage cavity and other defects. The pouring
The results show that tempering temperature has obvious effect on the quantity and morphology of carbides in 30cr13nb0.1 steel, which
The effect of tempering temperature on the impact properties of 30cr13nb0.1 steel is shown in Fig. 1. It can be
It can be seen from the figure that with the increase of tempering temperature, the hardness of 30cr13nb0.1 steel first
Fig. 1 shows the microstructure of 30cr13nb0.1 steel tempered at different temperatures. It is preliminarily judged that it is martensite
Test material and heat treatment process The ingot containing 0.117% Nb (mass fraction) was melted in 15 kg medium frequency
30cr13 martensitic stainless steel has good mechanical properties, hardenability and corrosion resistance, which is widely used in medical devices, measuring
1.Characteristics of wear resistant steel ball The composite wear-resistant casting steel ball has excellent comprehensive properties such as high strength,
The steel ball used in ball mill can be divided into casting ball and forging ball. Generally, the diameter of
The properties of tensile samples were tested by a universal testing machine controlled by microcomputer, and the tensile strength and
Six groups of samples were taken when analyzing surface carburization, and the location of the test point was changed to
In this test, 6 test pieces were poured in the same ladle of molten steel. The chemical composition of molten
In order to study the carburization defects of steel casting for bridge support, four sampling locations are selected, namely, near
Firstly, the mechanism and manifestation of carburization defects in steel castings are described, and then the experimental methods and main
The filling process of lost foam casting is the replacement process of metal liquid and foam pattern. Because the pouring
In order to study the impact resistance of steel castings at different temperatures, three temperature detection conditions, namely normal temperature,