Strength calculation and analysis of improved hydraulic valve body with shrinkage cavity
1. Casting valve body model with shrinkage cavity and calculation parameters There are two shrinkage cavities in the valve body […]
1. Casting valve body model with shrinkage cavity and calculation parameters There are two shrinkage cavities in the valve body […]
Yang Jinsong and Yu Lihua of Huazhong University of Science and Technology have studied the process of sand core of
The design of the pouring system is introduced by taking a combined hydraulic valve body as an example. The closed
1. Grid division In the AWB platform, the patch independent method is used to divide the tetrahedral mesh. At the
As one of the key components in the hydraulic transmission system, the working environment of the hydraulic valve is extremely
The hydraulic valve body of MXA-300 shearer is designed and manufactured by means of casting oil duct in coal mine
The so-called pouring system refers to the general name of the channel that guides the molten metal into the mold
Although the shape of the hydraulic valve body casting is simple, its quality differs greatly and the section structure is
With hydraulic valve body as carrier, the filling and solidification process of valve body casting were studied by combining theoretical
As a high load precision machinery, hydraulic components not only need to achieve accurate hydraulic transmission and control, but also
Hydraulic valves are subjected to complex and variable loads during their operation. Therefore, the strength of the valve body must
As one of the key components in the hydraulic transmission system, the working environment of the hydraulic valve is extremely
Based on one hydraulic valve body and two hydraulic multi way valve body, the design method of casting and pouring
Hydraulic casting valve is the main component of hydraulic system, which controls the pressure, flow and direction of oil in
In the process of casting simulation, the pouring system, grid division and calculation conditions are the same as the above,
1.Selection of gate valve body blank This method is suitable for the high pressure self tight seal gate valve body
As a high load precision mechanical part, the hydraulic valve body has the requirements of high pressure resistance, fatigue resistance
1) The blank of gate valve body is used to process the block valve to avoid opening the block valve,
As the isolation device of the overall hydraulic test of the boiler unit in the power plant, the hydraulic test
1.Requirements for casting material The composition and mechanical properties of the real object shall meet the standards specified in the
In casting production, the word “quality” has two meanings. The first is the quality of the casting itself, that is,
Because of the particularity of the working condition of nuclear power valves, the internal quality requirements of castings are very
Take the valve body as an example to briefly introduce the casting process design. 1.Selection of pouring position and parting
During the continuous cooling process after solidification, if the solid shrinkage of the casting is obstructed by Yin, the internal
The research team of ZHY casting decided to open the sand casting test mold first to verify the material fluidity
Casting refers to the process of heating the cast metal to the molten state to meet the requirements of certain
Formation of casting shrinkage cavity and shrinkage cavity during the solidification process of liquid metal in the mold, due to
There are not many components of the valve, ranging from several to dozens. These parts are generally divided into metal
In the process of solidification and cooling of sand-clad iron mold casting for pump valve castings, there are many cores
The production practice of iron mold sand covered casting pump valve castings shows that the iron mold sand covered casting