Grid division of centrifugal casting for super large high molybdenum cast iron cylinder liner
Man28-33d wet cylinder liner is selected as the research object. The blank length of cylinder liner is 686mm and the […]
Man28-33d wet cylinder liner is selected as the research object. The blank length of cylinder liner is 686mm and the […]
Through the analysis of the problems in the actual production of the original lost foam casting process and the ProCAST
1. Tendency shrinkage defects of gray iron castings after processing In the process of design and development of gray iron
1. Metallographic comparison The metallographic structure comparison before and after the improvement of the process of producing nodular cast iron
1. Molding process The two box core molding is adopted, and the sand filling core under the side molding is
Figure 1 shows the simulation of velocity field of molten metal. It can be seen from figure 1A that the
Engine is the power source of automobile and ship, and cylinder liner is one of the core components of engine.
The numerical simulation of lost foam casting filling process is shown in the figure. The whole filling process is stable
In casting production, due to the uneven wall thickness of the gray cast iron cylinder head, it is easy to
CB2 cast steel is a 9%~12%cr martensitic heat-resistant steel with a composition of 0.13c-9cr-1.5mo-1co-vnbnb, which is obtained by reducing C,
CB2 cast steel is a heat-resistant steel developed for 630 ℃ ultra supercritical units in the European joint research project
C Si Mn P S Cu Sb Mgincomplete 3.43 2.09 0.42 0.020 0.010 0.65 0.005 0.045 According to the above
The characteristic of rotary disc sand mold casting is rectangular. The internal and external shapes of rotary disc sand mold
1. White mold making Due to the large size of the vacuum pump shell casting, the white mold of the
The flatness of compacted vermicular cast iron platen surface is also very high. Therefore, the deformation of compacted vermicular cast
The internal shrinkage porosity and shrinkage cavity of the casting produced by the original lost foam casting process is relatively
1. Casting process Adopt the core assembly and vertical pouring process, pre assemble the base core, water jacket core, airway
1. Numerical simulation of bottom pouring inclined gating system in sand mold casting AnyCasting is used for numerical and simulation
In order to verify whether the top pouring process is reasonable, whether the molten iron mold filling can ensure the
1. Spheroidizing treatment Graphite distortion and fragment graphite will be produced in nodular cast iron with thick and large section
The solidification characteristics of heavy section nodular cast iron castings are: short liquid solidification time, long eutectic solidification time, and
Figure 1 shows the relationship between the tensile strength, Brinell hardness and w (TI) content of the test sample, in
The working surface of the composite roll is the outer surface, that is, the outer layer should meet the requirements
Whether the selection of mathematical model is reasonable or not directly imagines the accuracy of the whole simulation process, which
The tensile strength of gray cast iron cylinder head body is required to reach 300 MPa, and the tensile strength
The structure of special alloy gray cast iron frame gray cast iron used in the power system of high-speed railway
Based on the current manufacturing and use status of CB2 steel castings, in order to grasp the quality differences between
1. Analysis of sand casting process The material of sand mold casting rotary disc is HT250, which is a medium-sized
The front axle is a key component of the shock absorber system of an agricultural machine. It is usually produced
Furan resin sand is used for three box modeling, and the parting method is shown in Figure 1. See Figure