Simulation results and analysis of shrinkage porosity and shrinkage cavity in sand casting of mud pump body
Shrinkage porosity and shrinkage cavity are the most common defects in the process of sand casting, and they are also
Shrinkage porosity and shrinkage cavity are the most common defects in the process of sand casting, and they are also
Tractor transmission system is the core component of tractor, which determines the performance of the whole machine, reflects the manufacturing
1. Original mold design structure The original mold structure design of t9000-c iron mold sand coated casting cylinder block in
In order to reconfirm the defects of the nodular iron casting and the rationality of the analysis results, the CAE
At present, the manufacturing development of domestic tractor products and parts has the following characteristics and trends: 1) The average
The structure of gearbox shell is shown in Figure 1. Its material is QT500-7, the blank weight is 458 kg,
1. Casting process In order to ensure the smooth filling of molten iron and prevent the occurrence of defects such
The three-dimensional models of casting, sand mold and cold iron are meshed by finite element method. After being imported into
Dieless casting refers to the manufacturing of sand mold cavity for casting, which no longer uses molds. It has the
1.Selection and implementation method of inoculant Aiming at the problems of high pouring temperature and easy decay of inoculant in
Through the verification of small batch production, from the statistical table of defects, the first defect type is blow hole
Motor housing is one of the most important components of electric vehicle motor. ZHY casting produces a motor shell blank,
The cold extrusion process of spur gear is a net forming or near net forming process. Its production efficiency and
1. Water glass sand mold pouring test Figure 1 shows the water glass sand mold pouring test of the brake
In the manufacturing of mechanical parts, generally, the blank is generated by forming technologies such as casting, forging, welding and
The chilling effect of the cold iron will change the local cooling rate of the steel casting, so that the
The multi-element alloy additive is developed and designed by China Yituo on the basis of previous application experience according to
Six groups of samples were selected and tested for mechanical properties by wav-600a universal testing machine. The results are shown
Figure 1 shows the simulation results of filling sequence and velocity field of each part of mud pump body in
Developed countries carried out the research on the machinability of gray cast iron as early as the 1940s. After long-term
After analyzing the hot spot position and feeding channel of steel castings, the position of riser can be determined. In
With the help of ProCAST software, the temperature field and flow field in the filling process, temperature field and stress
In order to evaluate the rationality of the optimized process scheme, the software ProCAST needs to be used to simulate
The chemical composition of nodular graphite casting not only directly affects the mechanical properties of nodular graphite casting, but also
Compared with the traditional wood mold turning process, the mold size and size are limited by the table size and
Generally speaking, the riser should be set at the hot joint of steel castings, that is, the final solidification area.
The important roll part of an equipment, which was originally a welded part, is now changed into a ductile iron
The sand mold sand core of tractor complex castings adopts the methods of increasing material manufacturing and reducing material manufacturing
During solidification, the steel casting will produce liquid shrinkage and solidification shrinkage. When the feeding system cannot provide sufficient liquid
1. Pouring process selection According to the structural and functional characteristics of components, two feasible pouring schemes are determined before