Study on low cost and free cutting gray cast iron for engine cylinder block
With the development of thin-walled engine block, the engine bears higher and higher pressure, which requires higher strength and fatigue […]
With the development of thin-walled engine block, the engine bears higher and higher pressure, which requires higher strength and fatigue […]
The machinability of gray cast iron is affected by different melting methods. From a large number of research and tests,
Gray cast iron has the characteristics of low cost, good casting performance and shock absorption, The key to the further
(1) Fatigue test of ordinary HT250 lifting Faraday compression The lifting diagram of tension compression fatigue limit of ordinary HT250
The fatigue fracture process of metal casting includes fatigue crack nucleation and initiation, fatigue crack propagation and final instantaneous crack.
The tension compression fatigue fracture morphology of low alloy HT250 with different surface roughness is shown in the figure. Figure
In order to improve the properties of gray cast iron and deeply develop the application of gray cast iron, many
Results of tension compression fatigue test of low frequency gray cast iron Among the 8 samples of low-alloy HT250 low-frequency
Casting performance: it refers to some technological properties of whether the metal or alloy is suitable for casting, mainly including
The low magnification morphology of tensile fracture of three grades of gray cast iron is shown in Figure 1. It
Gray cast iron usually refers to the cast iron with gray section and the carbon mainly exists in the form
The tensile strength of ordinary HT250 at room temperature is slightly lower than the strength calibrated by its brand, which
Gray cast iron refers to the cast iron with flake graphite. The main components are iron, carbon, silicon, manganese, sulfur
The eutectic morphology of three grades of gray cast iron samples is shown in the figure. Eutectic clusters in gray
The matrix structure of three grades of gray cast iron samples is shown in the figure. It can be seen
1. Characteristics of inoculation treatment So far, there is no consensus on the action mechanism of inoculation treatment at home
The figure shows the graphite morphology and distribution of three grades of gray cast iron samples. It can be seen
1. Mechanical properties (1) Tensile strength: the tensile strength of gray cast iron is generally 100 ~ 350 MPa, which
The tension compression fatigue tests of three grades of gray cast iron are carried out on plg-100 high frequency fatigue
After the above WPS preparation, WPQR welding procedure qualification test shall be carried out to determine the WPS process reliability.
1. Melting process of alloy vermicular graphite cast iron for brake disc (1) Raw materials and chemical composition Pig iron,
Gray cast iron characterized by flake graphite has certain strength, hardness, elastic modulus, shock absorption, wear resistance and thermal conductivity,
The low-frequency tension compression fatigue test of gray cast iron adopts MTS810 axial tension compression fatigue test machine. It uses
From 2015 to 2019, the wind power market was constantly changing and experienced two rush loading peaks of wind power.
In the solidification process of liquid metal in centrifugal casting, too slow pouring speed will promote the formation of layered
Generally, the hardness of cylinder liner in the qualified layer is hb225 ~ HB240, and the overall hardness difference of
Based on all the previous analysis, the fracture process of nodular cast iron crankshaft is as follows: in the induction
The tension compression fatigue test of gray cast iron mainly studies the effects of loading frequency and surface roughness on
Casting refers to pouring molten metal into the mold, cooling and forming to form a casting that meets the relevant
1. Chemical composition control The chemical composition of nodular cast iron for wind turbine shall be strictly controlled, especially C,