Control of other elements in ductile iron
(1) Composition control and selection of as Cast Ferritic Nodular Iron: Micro hypereutectic composition, in which the carbon is slightly […]
(1) Composition control and selection of as Cast Ferritic Nodular Iron: Micro hypereutectic composition, in which the carbon is slightly […]
It is recommended that the optimum spheroidizing temperature range is 1420-1480 ℃, the spheroidizing temperature of nodular cast iron is
Through research and production practice, the following key problems must be solved in order to produce high-quality and mass qualified
Since the development and popularization of the process of producing crankshaft with iron film coated sand in the 1970s, due
① Increase the diameter of ladle nozzle and the size of gating system; ② Increase the number of ladle nozzles;
Although the application of shell casting in China is more than ten years later than that in foreign countries, it
The shell mold casting process of S1100 single cylinder diesel engine crankshaft was studied. S1100 single cylinder diesel engine crankshaft
Company profile: The Foundry Branch of Shanghai Diesel Engine Co., Ltd., located at No. 2636, Jungong Road, Shanghai, is a
Therefore, we analyze and sort out the causes of sand sticking in cast wear-resistant low alloy steel and the preventive
In 1940, Johannes Croning, a German engineer, invented the thermal method for manufacturing shell mold, which is called “C” method
There are many problems to be solved in the valve casting process, and relevant personnel should focus on the following
Crankshaft is not only the main key transmission part of engine, but also an important safety part. When the engine
(1) Super duplex stainless steel SAF2507 has good chloride stress corrosion resistance under low stress. Generally, 18-8 austenitic stainless steel
SAF2507 is the third generation of super duplex stainless steel, American Standard (national standard ZG 00Cr25Ni7Mo4N). Its microstructure has an
Experts and scholars at home and abroad have studied the application of numerical simulation technology in the fields of sand
(1) The simulation flow of numerical simulation software is introduced, and the setting of simulation parameters of reducer box body
The so-called pressure casting mainly refers to the aluminum alloy wheel hub casting obtained by filling the liquid metal into
How to overcome the shortcomings of quartz sand and significantly reduce the sand holes and pores of large and medium-sized
Company profile: Dongfeng Automobile Co., Ltd. Foundry Branch is located at No. 1, Checheng Avenue, Xiangfan City, Hubei Province, covering
At present, the manufacturing processes of excavator bucket teeth in China mainly include sand casting, forging manufacturing and precision casting.
According to the function of box casting, it can be divided into transmission box casting, pump body and valve body
The design of casting process of tractor reducer case is studied. The main research contents include the following parts: (1)
More than 100 years ago, Chernoff applied vibration during ingot forming, and the grain of ingot casting was refined. With
Numerical simulation of sand casting process is an interdisciplinary subject involving various disciplines such as information, materials, mechanics and computer.
The appearance forms of aluminum alloy casting hub mainly include coating and electroplating. Painting colors include sports silver and silver
“Pouring and solidification process” is a key process that has a significant impact on the quality of steel castings. More
Company profile: Dongfeng Motor Co., Ltd. commercial vehicle foundry No. 1 was founded in 1969, covering an area of 324000
The bucket teeth on the excavator are the combination of the tooth tip and the tooth seat (see Fig. 1
Most of the boxes are cast parts. The shape of box castings is generally complex. The main structure is cavities
Before the casting of valve castings, relevant personnel need to know the valve structure and valve overview in detail, such