Design principles of gating system for tractor box castings
The gating system of tractor box castings generally includes sprue cup, sprue, runner and inner sprue. Whether the gating system […]
The gating system of tractor box castings generally includes sprue cup, sprue, runner and inner sprue. Whether the gating system […]
The selected tractor reducer case is a large-scale casting designed by a company, which is produced in large quantities. It
Crankshaft is not only the main key transmission part of engine, but also an important safety part. When the engine
(1) Super duplex stainless steel SAF2507 has good chloride stress corrosion resistance under low stress. Generally, 18-8 austenitic stainless steel
The pouring temperature of cast iron is generally controlled between 1360 ℃ and 1450 ℃. In this paper, the pouring
SAF2507 is the third generation of super duplex stainless steel, American Standard (national standard ZG 00Cr25Ni7Mo4N). Its microstructure has an
Experts and scholars at home and abroad have studied the application of numerical simulation technology in the fields of sand
(1) The simulation flow of numerical simulation software is introduced, and the setting of simulation parameters of reducer box body
The so-called pressure casting mainly refers to the aluminum alloy wheel hub casting obtained by filling the liquid metal into
How to overcome the shortcomings of quartz sand and significantly reduce the sand holes and pores of large and medium-sized
As shown in Figure 1, it shows the filling flow state and temperature distribution at different times when the intermediate
In the casting forming of tractor box, if the parameters are set improperly, such as the mold cavity is too
Company profile: Dongfeng Automobile Co., Ltd. Foundry Branch is located at No. 1, Checheng Avenue, Xiangfan City, Hubei Province, covering
At present, the manufacturing processes of excavator bucket teeth in China mainly include sand casting, forging manufacturing and precision casting.
In order to study the distribution law of sand sticking sintering phenomenon in different parts of cylinder block, an experiment
According to the function of box casting, it can be divided into transmission box casting, pump body and valve body
The design of casting process of tractor reducer case is studied. The main research contents include the following parts: (1)
Molding materials play an important role in casting production. According to statistics, one ton of new sand is required for
The numerical simulation of sand casting defects is based on the temperature field and shrinkage cavity and porosity criteria during
Filling process is one of the main contents of sand casting process. Complex physical and chemical phenomena such as heat
The detection and analysis show that the main reason for the crack of the valve body is that it has
More than 100 years ago, Chernoff applied vibration during ingot forming, and the grain of ingot casting was refined. With
Numerical simulation of sand casting process is an interdisciplinary subject involving various disciplines such as information, materials, mechanics and computer.
The appearance forms of aluminum alloy casting hub mainly include coating and electroplating. Painting colors include sports silver and silver
In order to reduce the energy consumption of automobile and the pollution of exhaust gas to the environment, the development
“Pouring and solidification process” is a key process that has a significant impact on the quality of steel castings. More
Company profile: Dongfeng Motor Co., Ltd. commercial vehicle foundry No. 1 was founded in 1969, covering an area of 324000
The bucket teeth on the excavator are the combination of the tooth tip and the tooth seat (see Fig. 1
Most of the boxes are cast parts. The shape of box castings is generally complex. The main structure is cavities
Before the casting of valve castings, relevant personnel need to know the valve structure and valve overview in detail, such