Development direction of automobile exhaust system
With the improvement of engine efficiency and environmental protection requirements, it is required to improve the heat and corrosion resistance
With the improvement of engine efficiency and environmental protection requirements, it is required to improve the heat and corrosion resistance
The 13th five year development plan for foundry industry (hereinafter referred to as the plan) predicts that the medium and
In view of the change of exhaust temperature of automobiles, the materials used in the exhaust manifolds of automobiles are
With the development of the automobile industry, the exhaust temperature of the engine is increasing continuously, which leads to the
By controlling chemical composition, optimizing and improving the spheroidizing incubation process, the graphite grade and size of QT450-10 can be
Al-Cu system cast aluminum alloy is the earliest used casting alloy, which has high heat treatment effect and thermal stability.
1.Current situation Cast iron plays an extremely important role in China’s national economy and even in the world’s manufacturing industry.
Casting alloys must be melted first, then injected into the molds and cooled to the characteristics of the castings, making
At present, the majority of machine tool castings are still gray cast iron. The practice at home and abroad has
For a long time, the material of machine tool casting in China is gray cast iron, and the standard of
Due to the improvement of casting quality, casting precision, casting cost and casting automation, the future casting industry will develop
With the improvement of performance requirements of automobile parts for ductile iron parts, its material brand and performance exceed the
In the current economic development, the number of vehicles purchased by people and used for transportation is increasing day by
Squeeze casting technology has been used in the production of pneumatic instruments for many years. It is mainly used for
(1) The main causes of rear axle abnormal noise are as follows: The bearing is loose and damaged; the gear
The traditional method of high strength gray iron is to reduce the eutectic degree, to increase the austenite content and
Based on the above description of graphite distribution shape, the following conclusions can be drawn: (1) F-type graphite is only
In recent years, with the rapid improvement of science and technology level and the continuous promotion of industrial revolution, a
The common characteristics of special casting are: the casting size is accurate, the surface roughness value is low, closer to
Generally speaking, precision casting of automobile castings mainly refers to EPC and investment casting technology. With the development of automobile
1.Current situation Single crystal superalloy is the most important blade material of advanced gas turbine engine. China has made remarkable
1. Characteristics of inoculation treatment Up to now, there is no agreement on the mechanism of inoculation treatment at home
Full-mold casting refers to the casting method which uses polystyrene foamed plastic pattern instead of common pattern and pours metal
Among the special casting methods, metal mold casting and investment casting have the longest history. The real modern sense of
With the increasing requirements of energy saving, environmental protection and reducing the cost of components, large-scale structural casting of aluminum
1.Application in automobile and motorcycle casting As one of the main directions of piston blank production, squeeze casting has produced
Al-Si series alloy is the most widely used alloy system with the most varieties in cast aluminum alloy, and there
The chemical composition of grey cast iron is composed of two parts: one is the basic composition, i.e. the five
1.Current situation Aluminum and magnesium are typical light metal materials. Aluminum alloy has relatively light weight, high specific tensile strength
Among all kinds of casting methods, sand casting is the most common one. This is because it has many advantages: