Effect of vanadium or copper on high temperature tensile properties of high nickel austenitic cast steel for turbocharger shell
In order to ensure the performance of turbocharger shell at 1050 ℃, a high nickel (20wt%) austenitic steel ASTM HK40
In order to ensure the performance of turbocharger shell at 1050 ℃, a high nickel (20wt%) austenitic steel ASTM HK40
There is no doubt that the equipment demand of sandstone industry will increase substantially. However, there will be some new
The first piece appraisal meeting for the first stage stationary blade casting of 300MW class F heavy-duty gas turbine was
The increase in length of high silicon molybdenum ductile iron when it is cooled to room temperature after holding for
Although the amount of magnesium used in automobile industry is increasing, its application in automobile is still limited. At present,
1 Preliminary test As the pores are non fissured, N2 pores are excluded. In order to reduce the source of
The relationship between length increment and holding time of high nickel ductile iron at different operating temperatures is shown in
Although the macroscopic changes of the ductile iron studied are not obvious, the corrosion surface is slightly uneven after enlarged
In the future, titanium alloy precision forming technology will be developed to the direction of digitalization, informatization, automation and environmental
1. Defect category identification According to the shape and location of the stoma, the defect was initially identified as subcutaneous
Beijing Baimu aviation materials Hi Tech Co., Ltd. is a specialized manufacturing platform for titanium alloy casting materials and process
Automotive exhaust is mainly composed of CO, CH and NOX. It directly discharges into the air not only pollutes the
1. Current situation Material physical parameters are the direct basis of digital casting, which play a decisive role in the
The red oxide layer of high nickel ductile iron covers the surface of the sample while holding for 80 hours
1. Production process The 693 brake caliper and 812 brake caliper of ZHY casting are produced in the same line,
Fig. 1 shows the microstructure of high silicon molybdenum ductile iron after different thermal cycles at the upper temperature of
Titanium alloy has many advantages, such as low density, high specific strength, high temperature resistance, corrosion resistance, weldability and so
Before molding, assemble the core box according to the requirements, pay attention to the assembly sequence and the positioning of
In the 21st century, China’s squeeze casting technology will develop steadily and rapidly. Mainly reflected in the squeeze casting theory
With the continuous progress of society, atmospheric warming and environmental pollution have attracted more and more attention around the world.
Subcutaneous porosity is a common casting defect of nodular iron castings. The moisture in molding sand, resin in sand core,
Alloy cast iron is an iron-carbon cast alloy with some other elements added. It is often made by melting some
Ductile iron is commonly used to make structural parts on mechanical parts and equipment, mainly due to its relatively low
China’s foundry industry has been developing steadily since the 12th Five Year Plan, but its growth rate has slowed down
The as-cast microstructure of high nickel ductile iron observed under a microscope is shown in the figure.The graphite spheroidization of
1.Analysis of the reasons for the failure of the original process 1.1 cause analysis of shrinkage and porosity The riser
The strength of gray cast iron is mainly determined by graphite shape, size, pearlite in matrix and ferrite proportion. With
The figure shows the original as-cast structure of high silicon-molybdenum ductile iron. From Figure a, it can be seen that
The structure of the material determines the performance of the material, and the matrix structure of the material is often
1. Understanding of Squeeze Casting Technology As a process technology, squeeze casting has been widely used in production, but many