Internal stress, deformation and crack in valve casting
During the continuous cooling process after solidification, if the solid shrinkage of the casting is obstructed by Yin, the internal
During the continuous cooling process after solidification, if the solid shrinkage of the casting is obstructed by Yin, the internal
Large wear-resistant plate is a kind of wear-resistant steel parts, the amount of which is second only to grinding. Among
The volume fraction (3.3% – 4.6%) of M7C3 carbide calculated from two-step thermokinetics corresponds to the result (3.6% – 4.8%)
At present, the application of magnesium profile and deformation magnesium alloy in automobile is less (the average magnesium consumption is
1. Application abroad Volkswagen is the first automobile company to apply magnesium alloy on a large scale in automobiles. As
The research shows that about 75% of the fuel consumption is related to the vehicle mass. Reducing the vehicle mass
The research team of ZHY casting decided to open the sand casting test mold first to verify the material fluidity
Shrinkage is the physical nature of the alloy. Under normal pouring temperature, the shrinkage volume of the alloy with fixed
1. Electrochemical test The results of electrochemical polarization test of grey cast iron and nodular cast iron are shown in
ZHY casting takes a new type of alnbb refiner for casting aluminum alloy as the research object, and uses optical
Ball mill is the key equipment for grinding materials. It is widely used in silicate products, such as new building
Since the 12th Five Year Plan, China’s foundry industry has continued to develop steadily, but its growth rate has slowed
ZHY casting once produced 750 large-scale nodular cast iron pump body for customers. Figure 1 shows the casting drawing. The
Casting refers to the process of heating the cast metal to the molten state to meet the requirements of certain
Formation of casting shrinkage cavity and shrinkage cavity during the solidification process of liquid metal in the mold, due to
The mass fraction of carbon in iron is higher than 2%, while that of silicon is between 1% and 3%.
1 Smelting process First, scrap steel and pig iron are added to the 500 kg acid intermediate frequency electric furnace
At present, the chemical composition of the mainstream high chromium cast iron at home and abroad are: carbon 2.4% –
The progress of machine tool casting in China in the past 30 years can be seen in China International Casting
Lost foam casting and sand mold casting are two major processes in the foundry industry. They have both advantages and
In power station, petrochemical industry, metallurgy, ship industry and equipment manufacturing industry, there are large-scale bearing pedestal applications, such as
There are not many components of the valve, ranging from several to dozens. These parts are generally divided into metal
1.Shrinkage in the process of solidification and cooling, the reduction of volume and size is called shrinkage. Shrinkage is the
The advantages and disadvantages of machine tool casting are closely related to the machine tool industry and machinery manufacturing industry
The ball mill for cement industry mainly uses two kinds of wear-resistant products, namely grinding ball and lining plate. In
With the development of China’s economy, automobile, energy, ship, aviation, railway and other fields which are closely related to the
1 Rapid investment casting Investment casting, also known as “lost wax casting”, has a long history in China. It is
Pure metals are rarely used in casting production, and various alloys are generally used. In addition to the mechanical properties,
Micro morphology of worn surface The metallographic structure of the wear surface of the high chromium lining plate was observed
Graphite in grey cast iron is flaky, and its distribution shape can be divided into a, B, C, D, e