Spheroidizing quality of crankshaft cast iron
Magnesium is the main graphitization element, and the spheroidizing ability of rare earth is only one third of that of
Magnesium is the main graphitization element, and the spheroidizing ability of rare earth is only one third of that of
1. Design of formwork thickness The following contents shall be considered in the design of formwork: (1) the mold shell
The top pouring system of sand mold casting for tractor box adopts rain pouring, which is divided into four oval
The production of crankshaft blank by wet mold sand process is still the main traditional casting process, while the representative
A new type of cylinder block EA888 is a high-end sand casting. Due to its complex structure and wall thickness
The weight of tractor box castings is 205KG, and the estimated gating system mass is 20kg. According to the manual,
The choke cross-sectional area, i.e. the cross-sectional area of the ingate, is designed according to the choke section method. After
The gating system of tractor box castings generally includes sprue cup, sprue, runner and inner sprue. Whether the gating system
The selected tractor reducer case is a large-scale casting designed by a company, which is produced in large quantities. It
The pouring temperature of cast iron is generally controlled between 1360 ℃ and 1450 ℃. In this paper, the pouring
As shown in Figure 1, it shows the filling flow state and temperature distribution at different times when the intermediate
In the casting forming of tractor box, if the parameters are set improperly, such as the mold cavity is too
In order to study the distribution law of sand sticking sintering phenomenon in different parts of cylinder block, an experiment
Molding materials play an important role in casting production. According to statistics, one ton of new sand is required for
The numerical simulation of sand casting defects is based on the temperature field and shrinkage cavity and porosity criteria during
Filling process is one of the main contents of sand casting process. Complex physical and chemical phenomena such as heat
The detection and analysis show that the main reason for the crack of the valve body is that it has
In order to reduce the energy consumption of automobile and the pollution of exhaust gas to the environment, the development
Through magnetic particle testing, it was found that there were multiple cracks on the shoulder behind the furnace on the
The molten metal is poured into the hollow mold and cooled to form a product with the desired shape. This
German EB company is a famous foundry enterprise in the foundry industry. It is a family factory with a history
1. Pattern making The quality of pattern is one of the keys to the success or failure of lost foam
The counterweight iron material is HT100, and the structure is shown in Figure 1. It is a “bread” shape, on
Lost foam casting technology is made of polystyrene foam through the foaming process and the shape of the needed castings.
High pressure valve is one of the main parts of oil and gas production wellhead device, and its body structure
The casting simulation software ProCAST can predict the casting defects such as shrinkage porosity, shrinkage cavity and slag inclusion in
The process scheme is put into production after being determined by casting CAE simulation, and all valve castings are qualified
The alloy element Cr content of cf8c material is high. The high melting point of Cr increases the liquidus temperature
Although there are differences in local structure of valve castings of hydrocracking unit, the common structural feature is that the
The working environment of valve castings for petrochemical industry has the characteristics of high temperature, high pressure and hydrogen (including