Research status of wear resistant cast iron
1. Ordinary white cast iron Ordinary white cast iron can only be used in as cast state, and carbon atoms
1. Ordinary white cast iron Ordinary white cast iron can only be used in as cast state, and carbon atoms
1. Test scheme design Select specific nodular cast iron and specific process as the test object (as shown in Figure
Shrinkage porosity and shrinkage cavity are the most common defects in the process of sand casting, and they are also
1. Original mold design structure The original mold structure design of t9000-c iron mold sand coated casting cylinder block in
In order to reconfirm the defects of the nodular iron casting and the rationality of the analysis results, the CAE
1. Casting process In order to ensure the smooth filling of molten iron and prevent the occurrence of defects such
The three-dimensional models of casting, sand mold and cold iron are meshed by finite element method. After being imported into
Through the verification of small batch production, from the statistical table of defects, the first defect type is blow hole
1. Water glass sand mold pouring test Figure 1 shows the water glass sand mold pouring test of the brake
Six groups of samples were selected and tested for mechanical properties by wav-600a universal testing machine. The results are shown
Figure 1 shows the simulation results of filling sequence and velocity field of each part of mud pump body in
In order to evaluate the rationality of the optimized process scheme, the software ProCAST needs to be used to simulate
Compared with the traditional wood mold turning process, the mold size and size are limited by the table size and
The sand mold sand core of tractor complex castings adopts the methods of increasing material manufacturing and reducing material manufacturing
During solidification, the steel casting will produce liquid shrinkage and solidification shrinkage. When the feeding system cannot provide sufficient liquid
The structure of tractor castings is complex. For example, the transmission case shell part of chassis is a thin-walled shell
Finally, it enters the finishing stage of sand casting mold template, in which the part cutting allowance is set to
Figure 1 and Figure 2 respectively show the graphite morphology and matrix structure of two kinds of gray cast iron
As shown in the table, the mechanical properties of gray cast iron poured in two different heats are shown. It
When the rotating speed and feed rate are constant, the cutting length of the cutting edge for cutting each sample
The solid models of sand mold casting, sand core, sprue and riser are made in the form of part modeling.
Riser refers to the structure artificially set in the pouring and riser system to store metal liquid. In the pouring
1.Graphite morphology Figure 4 shows the graphite morphology of two groups of gray cast iron samples. It can be seen
Sand casting molds mostly belong to the blank mold of casting products, and the template is a part and the
1. Structure description of sand casting coupling parts Based on the above reasons, this topic adds the working condition mechanical
When the rotating speed and feed rate are constant, the cutting length of each sample cut by gray cast iron
The influence of reassembly of the same blade at different cutting depths on the cutting force is shown in the
One of the important physical parameters in the process of cutting gray cast iron is cutting force. In the process
Shrinkage cavity in sand casting is a common casting defect, which is basically a volume loss defect. According to the
In the gray cast iron cutting force measurement test, the different installation position of the turning tool and the sticking