Optimization of impeller casting process based on AnyCasting
Based on AnyCasting, the process simulation and optimization of large aluminum silicon alloy casting impeller are carried out, and the
Based on AnyCasting, the process simulation and optimization of large aluminum silicon alloy casting impeller are carried out, and the
Impeller casting has excellent mechanical properties: no hot crack tendency, good impeller casting performance, small linear shrinkage, easy recovery and
According to the solidification sequence of impeller casting, the timely feeding of riser can not be obtained at the thick
Draw the 3D pouring model of impeller casting process in Pro / E software, output STL file, and import it
Because the cast impeller is a medium-sized casting, its structure is relatively simple, and it is mass production. Its parting
The shape and dimension inspection of impeller casting is to check whether the actual dimension of impeller blank casting falls
In view of the current situation that the production quality of large and complex integral stainless steel casting impeller can
Due to the thin and large number of impeller blade castings, in order to further inspect the surface and near
According to the number of blades of this kind of impeller, the complexity of structure and the technical requirements of
The surface roughness of cast impeller refers to the micro geometric characteristics composed of micro spacing and peak valley on
The surface defects of impeller castings are first inspected by visual observation, in which a 5x magnifying glass is also
According to empirical parameters, when the wall thickness of impeller investment casting sand casting is > 40 mm, the minimum
Because the investment mold of impeller blade is fixed with rosin wax based mold material and sodium silicate sand sleeve,
The quality of investment casting directly affects the geometry, dimensional accuracy and surface roughness of investment casting impeller. When investment
a. Research status of casting technology of small and simple impeller For the casting impeller with small size, light weight
1. Selection and determination of detection method As a key part of the pump body, the impeller of desulfurization pump
The surface of the blade of the sulfur pump impeller and the surface of the blade are calculated to achieve
Coating configuration and drying is one of the important links to obtain high quality castings. The role of sand casting
It is beneficial to obtain castings with clear contour, precise shape, smooth surface and intact internal structure by mastering the
Before molding, assemble the core box according to the requirements, pay attention to the assembly sequence and the positioning of
1. Foam mold size determination The design of foaming mould mainly includes the following aspects: determining the size parameters of
The production impeller adopts the EPC resin sand composite molding process to obtain the whole sand core, which improves the
The production difficulty of impeller mainly lies in the whole molding process. Using traditional casting technology, it is difficult to
Technical requirements for impeller production (1) The surface of the casting shall be smooth and free from defects such as