Effect of pouring speed on the quality of sand castings
The pouring speed is also an important factor affecting the quality of sand castings. If the pouring speed is too […]
The pouring speed is also an important factor affecting the quality of sand castings. If the pouring speed is too […]
Various cast iron codes are composed of the first capital letter of the Chinese pinyin letter representing the characteristics of
There are two main forms of incomplete forming of bucket teeth in Squeeze Casting: incomplete bucket teeth and incomplete forming
Nodular cast iron is a high-strength cast iron material developed in the 1950s. Its comprehensive properties are close to steel.
Through the simulation analysis of mold filling and solidification process of different pouring schemes, the similarities and differences of mold
1.How to control the pouring temperature? Since lowering the pouring temperature has so many advantages, how can we ensure smooth
The application of sand casting coating can close the pores between sand particles on the surface of mold and core,
The molten steel contains gas in the melting process, which requires pre deoxidation and final deoxidation. If the deoxidation is
(1) There should not be too much recycled sand in the core sand, because there are too many fine sand
Company profile: Yuchai Machinery Co., Ltd. is the largest professional diesel engine manufacturer in China. The foundry is its cost
Sand casting is the most popular and simplest type of casting, which has been used for centuries Sand casting is
More than 80% of the products in the foundry industry are made by sand casting, so we usually refer to
In order to ensure the quality of castings, the core used in sand casting is generally dry core. The clay
Sand and molding sand are the basic raw materials for casting. The most commonly used casting sand is siliceous sand.
Bucket teeth are the key vulnerable parts of mining excavators. Their working objects are generally ore, rock or soil. The
The influence of carbon and silicon content on the quality of nodular iron castings is shown in the figure below:
China has a vast territory, vast territory and abundant resources, rich and complete types of mineral resources, and open-pit mining
Porosity is one of the most common casting defects in castings. According to the different formation mechanism, it is mainly
(1) Technical analysis of valve body castings: according to the requirements of user drawings, RT flaw detection shall be carried
Through production test and research, the following problems exist in shell casting process: (1) mold shell deformation: mold shell deformation
(1) carbon equivalent shall be increased as much as possible without causing graphite floating. After the test, the carbon equivalent
The process test of S1100 crankshaft shell in multiple batches is shown in the table. Serial number Material Pouring quantity
Carry out multi batch pouring and anatomical analysis on the shell cast crankshaft, and make corresponding adjustment and improvement: For
Squeeze casting technology continuously applies pressure to the liquid metal in the forming process, which makes the liquid metal solidify
The necessary condition for spheroidization is that magnesium as the main element in spheroidizing agent of nodular cast iron is
1. Melting, spheroidizing and inoculation treatment 1000kW medium frequency induction furnace is adopted for smelting, and the charge is 90%
The rear axle of the excavator is shell type and of high quality. The original process of the factory adopts
Figure 1 shows the filling process of the stepped gating system used in the sand casting of the tractor box.
Reducing pouring “temperature” to reduce sand hole and air hole defects of large steel castings Reducing the pouring “temperature” is
The rear axle of high-speed excavator is the installation device of differential and half shaft, and bears the counter torque