Shrinkage porosity and shrinkage cavity in steel castings
During solidification, the steel casting will produce liquid shrinkage and solidification shrinkage. When the feeding system cannot provide sufficient liquid […]
During solidification, the steel casting will produce liquid shrinkage and solidification shrinkage. When the feeding system cannot provide sufficient liquid […]
1. Pouring process selection According to the structural and functional characteristics of components, two feasible pouring schemes are determined before
The structure of tractor castings is complex. For example, the transmission case shell part of chassis is a thin-walled shell
According to the structural characteristics of sand casting mud pump body and the physicochemical properties of ZG35, two sets of
Combined with a specific case of large-scale steel casting processing and manufacturing, the application of modeless NC processing technology in
Finally, it enters the finishing stage of sand casting mold template, in which the part cutting allowance is set to
Figure 1 and Figure 2 respectively show the graphite morphology and matrix structure of two kinds of gray cast iron
Taking the sand mold casting of the mud pump body as the research object, according to the size and structural
Rapid Moldless mold processing and production driven by digitization is not only a common technology in modern industrial production, but
As shown in the table, the mechanical properties of gray cast iron poured in two different heats are shown. It
First perform rough machining of sand casting mold template, create a tool with diameter d = 40mm and fillet radius
In recent years, NC technology has developed rapidly. Developed countries have fully popularized NC machining and manufacturing technology in industrial
When the rotating speed and feed rate are constant, the cutting length of the cutting edge for cutting each sample
The solid models of sand mold casting, sand core, sprue and riser are made in the form of part modeling.
Riser refers to the structure artificially set in the pouring and riser system to store metal liquid. In the pouring
1.Graphite morphology Figure 4 shows the graphite morphology of two groups of gray cast iron samples. It can be seen
The low spheroidizing grade of lost foam casting nodular cast iron is mainly caused by high spheroidizing temperature (due to
Sand casting molds mostly belong to the blank mold of casting products, and the template is a part and the
1. Structure description of sand casting coupling parts Based on the above reasons, this topic adds the working condition mechanical
As a high-performance material, nodular cast iron has been widely used in many industries. After years of development, the output
When the rotating speed and feed rate are constant, the cutting length of each sample cut by gray cast iron
The pouring process of liquid metal involves the phase transformation process of metal. Even on the premise of meeting the
The influence of reassembly of the same blade at different cutting depths on the cutting force is shown in the
The tensile strength of gray iron castings has been increased from 200 MPa to 250 MPa or even 300 MPa.
When liquid metal is poured into the mold, it will produce volume shrinkage during cooling and solidification. This shrinkage may
The casting system of sand casting axle housing is simulated and analyzed by using ProCAST simulation software. The solidification sequence
As a key part of tractor, the main contents of sand casting axle housing are as follows: firstly, the structural
One of the important physical parameters in the process of cutting gray cast iron is cutting force. In the process
1.Purification degree of molten iron Some high melting point and high hardness particles remain in the molten iron and become
Shrinkage cavity in sand casting is a common casting defect, which is basically a volume loss defect. According to the