Technology of producing gray iron lost foam casting by using water slag iron ironmaking
Water slag iron is formed from the waste slag in the high-frequency steelmaking furnace by rapid cooling in water. It […]
Water slag iron is formed from the waste slag in the high-frequency steelmaking furnace by rapid cooling in water. It […]
The simulation software of lost foam casting simulation is ProCAST and visual environment. ProCAST can accurately simulate the flow process
After the molten metal is poured into the mold, it usually produces volume shrinkage in the process of solidification and
After determining the type and layout of the nodular cast iron gating system, it is necessary to calculate the specific
In the process of lost foam casting molding, solidification is the process of metal liquid gradually cooling from liquid phase
Among the many strengthening mechanisms, the method of grain refinement is the best way to control the strength and toughness
The function of sand core is to shape the hole, inner cavity or parts that are not easy to produce
Although lost foam casting has been successfully applied in the actual production of iron castings, the cognition and understanding of
When studying 00cr13ni5co9mo5 maraging stainless steel, Luo Jing et al. Found that only a small amount of martensite was transformed
According to the actual production situation of sand casting, on the basis of summarizing and analyzing the theory of sand
2Crl3 stainless steel is a hypoeutectoid steel. The temperature is raised to the austenite transformation temperature and kept for a
Li Yupeng and others found that under the same quenching and tempering process, the tensile strength of 2Cr13 Steel after
To design the process of nodular cast iron, in addition to selecting the correct casting method and process scheme, the
The main difference between lost foam casting and sand casting is that the molding process of lost foam casting no
Generally speaking, as cast alloy steel is mostly ferritic + carbide phase, so is 2Crl3 stainless steel, which needs further
The tempering process is a quenching and tempering step after the previous heat treatment. Although the martensite in the structure
The selection of parting surface is directly related to the dimensional accuracy, production cost and efficiency of nodular cast iron.
Lost foam casting is formed by foamed plastic beads (EPS, EPMMA or STMMA) after foaming and molding in the mold,
At present, the application of computer in simulation casting process mainly focuses on the following aspects: (1) Simulation of mold
There are many classification methods of stainless steel materials: austenite, martensite, ferrite and dual phase structure; There are chromium and
(1) Development of water-based quick drying and self drying casting coatings The water-based casting coating has the advantages of low
According to the actual production situation, the automobile hub support casting is produced by using the Japanese Xindong automatic pouring
Relevant research in China began in the late 1970s. Although it started late, it developed rapidly. In 1980, Shenyang Foundry
The traditional heat treatment method of 2Crl3 generally recommends 1000 ° c-1050 ° C oil cooling or water cooling +
Due to the development and improvement of the output and technical level of China’s steel industry, the demand and standard
Gray cast iron is the most widely used cast iron at present. It is named for its gray section color.
Spheroidizing treatment and inoculation treatment are essential pre furnace treatment steps for raw molten iron of nodular cast iron. The
As early as 1940, computer technology had just started. Victor paschkis of Columbia University in the United States put forward
Water slag is formed by rapidly cooling the blast furnace slag in the hot-melt steel-making high-frequency furnace in water. There
In order to obtain as cast ferrite pearlite nodular cast iron with high strength and good plastic toughness, the production