Operation procedure: Preparation: 1) Check the condition of furnace body: check whether the furnace lining, copper tube induction coil, cooling […]
Operation procedure: Preparation: 1) Check the condition of furnace body: check whether the furnace lining, copper tube induction coil, cooling […]
This paper mainly carries out scheme design, simulation analysis and production verification of a kind of bridge bearing steel casting,
Figure 1 is a plot of the mass gain per unit area of a high temperature alloy sample prepared at
Relying on ZHY casting, the company is a medium-sized private enterprise producing bridge bearing steel castings. The transfer casting process
Operation procedure: Check whether the baking furnace and temperature control meter are normal and whether the furnace bed is flat
Fig. 1 is the curve of mass added value per unit area of Superalloy samples prepared at different pouring temperatures.
Operation procedure: Equipment preparation: 1) The pressure of steam generator for dewaxing shall be 0.8-1.0mpa, and the minimum pressure shall
1. Test materials The test material is superalloy K4002 Sr. When 0.4-0.6% SR is added to the alloy, the chemical
Operation procedure: Before coating and hanging the surface layer, check whether the cleaned module has dropped parts, and check whether
Based on the use of bucket teeth in production, according to the components of bucket teeth, they can be divided
The superalloy can work at 760 ~ 1500 ℃ for a long time and bear certain stress. Because the superalloy
After the casting spheroidization problem appeared, our company’s technical, quality, physical and chemical department and other departments jointly analyzed, according
Operating procedures: a) Before assembly and welding, visual inspection shall be carried out for all wax molds again to remove
1. Improvement of structure From the actual failure of the bucket teeth, it is found that the tooth tip is
On the basis of the existing research, there are still many works to be further improved and upgraded. In particular,
After the occurrence of bad nodularity, our plant strengthened the detection of sulfur in the original molten iron and the
Operation procedure: Before wax repair, check the wax mould that has been cooled and has no defects in appearance. For
1.Simulation results and analysis of filling process The filling process of multi way valve casting is as shown in the
The bucket teeth need to bear the impact and bending moment from the material when contacting the material. During the
Excavator is a common important construction machinery, which is widely used in many industries of national economic construction, and plays
The hydraulic valve is an essential component in the hydraulic system. The performance of the hydraulic valve determines the performance
In the production process of nodular iron castings, in order to ensure the product quality, the tensile strength, yield strength,
1.Casting system model of double hydraulic valve body The design method of the valve body gating system is similar to
Taking the simplified one hydraulic valve body and the two multi way valve body for loader as the research object,
Liu Hanwu and others of North China University of Science and Technology studied the stress and strain of two-way cartridge
The drawing shows the shrinkage pore distribution of a series of hydraulic valves made of steel-304 stainless steel with casting
ProCAST software uses finite element method to simulate heat transfer, filling flow process, thermal-stress coupling field, microstructure and shrinkage cavity.ProCAST
1.Partial differential equation for heat conduction: The solidification process of castings is a complicated phase transition process.Solidification is a dynamic
Wang Min and others from Harbin Harbin Harbin Boiler Valve Co., Ltd. take DN300 and PN25 cast valve bodies as
This control procedure is applicable to the routine pouring of the company and is used as the guidance document for