Principle and technology of thin wall casting by vacuum differential pressure casting
In order to meet the requirements of lightweight and integration of components, a large number of large-scale complex thin-walled aluminum
In order to meet the requirements of lightweight and integration of components, a large number of large-scale complex thin-walled aluminum
In recent years, with the increasingly prominent global climate warming and energy issues, governments of all countries require automobile manufacturers
Develop large-scale cupola of more than 5t / h and adopt external hot air supply and water-cooled cupola without furnace
The aluminum alloy thin-walled shell casting is produced according to the actual engineering demand. After the production is completed, the
The key technologies involved in the digital chemical plant are: digital modeling technology, virtual reality technology, optimization simulation technology, application
Wheel tractor chassis fault usually has a more complex cause. If the manipulator can not identify the fault in time
Aluminum alloy plate technology is mature, lightweight effect is obvious, cost is relatively low, widely used in the body. Compared
Through the understanding of this defect, we start with the properties of molding sand and focus on the properties of
The gray iron casting of a certain type of automobile engine block has a maximum outline dimension of 371mm ×
According to the global casting production census conducted by modern casting magazine of American Foundry Association, in 2018, the global
Establish a new raw and auxiliary material system suitable for high-density clay molding sand, develop different kinds of raw sand
00bob cylinder is the key pressure bearing high temperature steel casting of supercritical steam turbine. Its function is to separate
In this design, a new aluminum silicon alloy is used as the shell casting material. By adding Al-10Sr modifier and
The establishment of digital foundry has many advantages, as follows: 1) Improve the quality of factory design Digital factory design
In order to alleviate the impact of human beings on climate change, energy efficiency of iron and steel enterprises has
Aluminum alloy extruded profiles are suitable for body middle beam structural parts. The structural design of the parts is flexible
Vacuum die casting is an advanced die casting technology, which can eliminate or reduce the defects such as air entrainment
With the increasingly stringent requirements of energy security and environmental protection, automobile energy saving and emission reduction has become an
With the goal of strengthening and toughening, lightening, precision and high efficiency, we should develop new cast iron materials, focus
With the economic development of the country, all walks of life are developing rapidly, and the machinery industry is also
Automation refers to the process of machine equipment, system or process (production, management process) without the direct participation of people
Among all the metal manufacturing processes, the biggest advantage of the casting process is that the chemical composition of the
On the whole, the academic research in the field of foundry in China is not backward, and many of the
Based on the analysis of the results of the improvement, the casting process can be further optimized to ensure the
In casting production, gating system is one of the important factors that affect the quality of castings. According to the
Automobile brake calipers are castings with compactness requirements. In practical application, defects such as shrinkage, shrinkage and porosity can not
If designing high-temperature stress components, such as water-free cooling furnace roller, the designer must consider the specific performance characteristics, because
(1) Global economic downturn, slow recovery The global economic situation is grim and complex. The weak demand in the international
In the face of the rapid development of information and technology in the world, and the rapid improvement of the
The riser design of cast steel joint mainly depends on the solidification characteristics of cast steel. There is a large