Classifications of iron casting
Iron casting refers to iron carbon alloy casting with carbon content less than 2.11% which is majorly made of foundry iron.
Iron casting refers to iron carbon alloy casting with carbon content less than 2.11% which is majorly made of foundry iron.
In foundry industry, there is a revolutionary method we call it V process casting. V process casting is invented in japan
The most important characteristics of Vacuum casting is that molding sand is dry sand without binder.This method molds the sand with plastic
Lost foam casting has several Characteristics below Firstly,flexible design of lost foam cast. Provides sufficient degree of freedom for casting
Chapter 1: The Introduction of Lost Wax Casting Lost Wax casting is a kind of precision casting , is also called
Chapter 1 : The Introduction of Investment Casting The so-called investment casting process , it is simply said that use fusible
Though lost foam casting started earlier in China, its progress has been slow. Until the early 1990s, it has carried
Lost foam casting is a casting process gradually developed later in the 1980s. it is a kind of new casting
Lost wax casting process is a very important part in the production process of investment casting. Under the function of
The technology of lost foam metal casting is developing very fast, but our country still has a certain gap than
Styrofoam casting is also called “gasification molding” , “polystyrene foam plastic casting” and so on. The essence of this casting
The Lost Foam Process, also known as the Evaporative Pattern Casting (EPC) process, is a modern and innovative technique used
Lost wax casting is one of the glass forming processes. The main content is heating glass to a very high
Lost foam casting pattern use the casting foam instead of the wax. The casting foam made from a material we
Using the foam casting, it can be more advanced compared to other casting ways. Coz the foam casting is a
Definition: Full mould casting (also known lost foam casting process) is a new kind of casting method. That is to
The development of casting steel industry and the improvement of steel-making technology are inseparable. Although the technology of wronght steel
Casting of iron had played a huge role in the process of human civilization. so far as one of engineering
Process of lost foam casting process can save cost and produce products with high quality,so it is widely used by
Lost Foam Casting has a very detailed process during its making. Firstly, we need to produce some empty foam model
China in 513 BC, cast the earliest written records of cast iron parts of the world – the state of
Our products are all manufactured in accordance with ISO9001:2008 international standards, so you can feel at ease in purchasing and
ZHY processes a research team led by domestic senior engineers who have been in this industry for many years, has
On November 7, the working committee of industrial cluster of China Foundry Association held the third annual meeting of China