Application effect analysis of high chromium cast iron in large autogenous mill liner
Select a mine φ 12.2 m × The middle ring liner of 11.0 m autogenous mill is taken as the […]
Select a mine φ 12.2 m × The middle ring liner of 11.0 m autogenous mill is taken as the […]
Combined with the rule of dimension error transfer from CAD model to one-time wax impregnation, the dimension shrinkage in X
Based on the rule of dimensional error transfer and reverse engineering, the 3D digital scanning of complex parts after one
Composition analysis of high chromium cast iron At present, the research of high chromium cast iron focuses on hypoeutectic or
In view of the influence of different post-treatment on the surface quality of the specimen, considering the low surface strength
Analysis of casting structure and casting process The main body of the lower half casting of the rear cylinder is
In the experiment, the dimension deviation is used as the measurement index of the dimension accuracy of the specimen. The
For the SLS fired specimens, the specific dimensions are shown in Figure 1. The size of the sample for selective
The process parameters of SLS were predicted as follows: temperature 95 ℃, laser power 30W, powder layer thickness 0.14mm, scanning
As for specimen selection, Wang Danni of Wuhan University of science and technology used finite element analysis and BP neural
The transformation of alloy from liquid to solid is called solidification, during which casting defects are concentrated. In the process
For SLS rapid prototyping process, it is difficult to achieve the SLS prototype with good surface quality and dimensional accuracy
In the selective laser sintering process, the process parameters have a great influence on the sintering quality. The main influencing
The delamination thickness of the model is mainly determined by the precision of the rapid prototyping equipment, the particle size
STL (stereolithography) was founded by 3D system software company. It was initially used in the early stereolithography machine to determine
Because the sintered materials are mainly thermoplastic polymer materials and their composites, under the action of laser, the powder absorbs
In SLS rapid investment casting process, there are SLS prototype preparation, SLS prototype post-processing and alloy casting solidification process, and
Based on the process of rapid investment casting, the source of dimension error in the process of rapid investment casting
Selective laser sintering (SLS) is also known as selective laser sintering (SLS). As a processing technology based on the idea
The experimental and modeling studies on the heat transfer behavior and pressure transfer law of the casting die interface in
The microstructure after heat treatment was observed and studied. It was found that there were various sizes of holes left
The displacement of casting is defined as the displacement of nodes caused by solidification shrinkage and punch pressing. As shown
As shown in Figure 1, the pressure nephogram of aluminum alloy and magnesium alloy castings at different times (the pressure
The comprehensive mechanical properties of 7075 alloy wheel parts in as cast and T6 states by rheo squeeze casting were
Figure 1 (A-D) and figure 1 (E-G) show the solidification of aluminum and magnesium alloy castings at different times during
Although rheo squeeze casting can improve and improve the mechanical properties of 7075 alloy parts and eliminate some macro segregation,
As shown in the figure, the casting die interface pressure reaches the maximum value soon after the applied pressure. The
The simulation method based on ANSYS is used to solve the temperature field and stress field in squeeze casting process.
In the process of squeeze casting experiment, the material of the casting is aluminum alloy and magnesium alloy. The shape
With the solidification process, the interface pressure gradually decreases to zero at some positions. When the interface pressure is reduced