Dewaxing of impeller shell in investment casting
Because the investment mold of impeller blade is fixed with rosin wax based mold material and sodium silicate sand sleeve,
Because the investment mold of impeller blade is fixed with rosin wax based mold material and sodium silicate sand sleeve,
The quality of investment casting directly affects the geometry, dimensional accuracy and surface roughness of investment casting impeller. When investment
Figure 1 and Figure 2 show the graphite structure of HT250 and HT200 gray cast iron under the conditions of
1. Sample preparation According to the requirements of GB / t9439-2010 lost foam casting gray iron castings, it is used
The effect of alloy element Mo on the thermal fatigue properties of gray cast iron was analyzed by comparing two
According to the three carbon source calculation models based on three types of sand casting process parameters, the total carbon
The effects of alloying element Mo on the microstructure and mechanical properties of high-strength gray cast iron were compared and
1.Effect of aging treatment For the engine parts of gray cast iron cylinder head, such as cylinder block, cylinder head,
Pour a positioning plate product. The maximum wall thickness of the casting is 90 mm, the minimum wall thickness is
In the process of thermal cycle, cracks caused by periodic stress due to internal temperature difference, hindered shrinkage and thermal
Casting defect Cause Improvement measures Increase or decrease in outer diameter The external mold shrinks and deforms, the direction of
The microstructure characteristics of gray cast iron determine its mechanical properties. For the microstructure of gray cast iron, the finer
The modifier used in the study is jf-1 modifier. In the experiment, the composition of gray cast iron and the
ZHY casting has developed a frame shell casting with material grade of HT250 and overall dimension of 1300 mm ×
Most gray cast iron castings can become machine parts only after turning. The turning performance directly affects the processing quality
The composition of the experimental gray cast iron and the types of inoculants added. By comparing and analyzing the effects
Adding alloying elements to cast iron can improve the strength of gray cast iron. The effects of manganese, some alloying
Adjust carbon equivalent and silicon carbon ratio. In the solidification of gray cast iron, the carbon equivalent directly affects the
Because there is no solid phase in the initial state of the mold cavity during the micro model calculation, and
At the same time, considering the pressure and speed in the filling process of lost foam castings, so far, the
The solidification process of sand castings is directly related to the shrinkage cavity, porosity and stress concentration of sand castings.
1. Sand core design of sand mold casting The core is made of furan resin self hardening sand. Because the
The spiral case is made of QT500-7, and its chemical composition is shown in the table. The production nature of
After the simulation calculation is completed, enter the visual viewer post-processing interface, observe the dynamic change of liquid metal temperature
The accuracy of the back calculation program needs to be verified. We select the difference between the measured temperature data
Compared with other metal castings, sand casting has the advantages of low cost, simple production process and short production cycle.
1. Simulation analysis of liquid metal filling process The filling state and temperature distribution at different stages of liquid metal
As shown in the figure, the porosity results of numerical simulation of nodular cast iron are mainly used to judge
Because the nodular cast iron of the hub support is the main body of the simulation, and its grid quality
The process of rapid sand casting technology to realize the rapid manufacturing of parts is as follows: establish the three-dimensional