Matters needing attention in casting process of ductile iron piston
The wall thickness of ductile iron piston varies greatly, the thinnest part is 7.5 mm, the thickest part is 23 […]
The wall thickness of ductile iron piston varies greatly, the thinnest part is 7.5 mm, the thickest part is 23 […]
Based on the actual casting cases of cylinder block castings collected from domestic foundry enterprises, combined with the existing achievements
The casting properties of ductile iron have the following characteristics ① The content of sulfide and oxide in molten iron
In the field of digital casting abroad, it is more reflected in the whole process automation of casting process. Kurtz
At present, in the field of digital casting, domestic research focuses on the development and application of digital casting database
The floating of graphite and abnormal shape of graphite in the center is a kind of metallographic structure defect associated
It has been proved by a lot of practice that the process design of gating system is the key problem
The State Key Laboratory of advanced forming technology and equipment of China Academy of Mechanical Sciences has systematically studied the
Material, mold, core making and inspection are the four basic aspects of engine block casting, which run through the whole
Large and medium-sized engine is an important power source of mechanical equipment, which is widely used in automobile, ship, engineering
Molding manufacturing technology can be used not only in functional testing, but also in product conceptual design, and also in
Layered solid manufacturing The foil of hot melt adhesive is painted on one side, and the parts are heated. In
The pillar industry of China’s economic development is the modern machinery manufacturing industry. In order to promote the sound and
Solid liquid segregation is one of the main defects in thick wall products. Under the condition of good feeding condition
The influence of process parameters on the shrinkage cavity and porosity in the semi-solid die casting process was studied by
In the process of analyzing the solid-liquid segregation, in order to identify the bright white cxal grains and the dark
Semi solid die casting is different from the traditional liquid die casting, which is mainly reflected in the different slurry
In this experiment, the method of controlling variables is adopted. The mold temperature is set as 230 ° C, 140
Shrinkage porosity defect is the key research object of this project. The observation method for this defect is fluorescence penetration
In this test, the control variable method is adopted, and the material handle thickness is set as 16mm, 31mm, 42mm
Vickers hardness measurement The unit of hardness measured is micro Vickers hardness. When hv-30 Vickers hardness tester is used, the
During the preparation of metallographic samples, sawing, cutting, grinding, polishing and other processes are required. After the blank samples to
In this test, the method of variable control was adopted. Under the condition of other parameters unchanged, the boosting pressure
(1) Aiming at the common shrinkage and porosity defects in semi-solid die-casting thick wall products, the microstructure analysis and mechanical
Solid liquid segregation is a typical semi-solid defect in thick wall products. It refers to the uneven distribution of solid
In semi-solid casting, in order to reduce or even eliminate the shrinkage cavity and porosity defect, the surplus slurry is
1 metallographic structure analysis The optical microscope (OM) used in this experiment is axiovert 200, and the magnification is 25,
The traditional liquid die casting metal from liquid solidification to solid state needs first liquid shrinkage in pure liquid state,
In the defect analysis of semi-solid thick wall products, shrinkage cavity and porosity are the typical defects studied. In the
Due to the characteristics of semi-solid slurry, semi-solid forming has the following natural advantages over other casting methods (1) In