Filling process and simulation analysis of molten metal in sand casting axle housing
In the filling process, the flow of molten metal will have a great impact on the quality of the axle […]
In the filling process, the flow of molten metal will have a great impact on the quality of the axle […]
As shown in the figure is the structure diagram of polished state of lzqt600-3 ductile iron section edge, 1 /
ProCAST casting computer simulation process: firstly, Creo software was used to establish the three-dimensional numerical model of the casting system
The corrtest electrochemical test system can automatically carry out the electrochemical corrosion test and fit the test curve. Before the
The gating system is the channel to guide liquid metal into the mold cavity in sand mold. Its structure is
The friction and wear tests of nitrocarburizing samples were carried out on a friction and wear testing machine. The friction
Numerical simulation is a method that uses the correspondence between different things to verify measures. Numerical simulation is irreversible. Casting
Casting process parameters mainly include dimensional tolerance, linear shrinkage, draft angle and other aspects. The determination of these process parameters
According to the statistics of pearlite content in the structure of nodular cast iron under corrosion state, the gray data
In the molding process of sand coated iron mold, sand collapse and empty shell are the important reasons for sand
The linear shrinkage of the bridge shell has a great influence on the accuracy of the size of the bridge
Generally speaking, the higher the pouring temperature is, the better the fluidity of alloy liquid is, and the more favorable
Spheroidization rate is one of the important and often used evaluation criteria of ductile iron. The calculation method is as
For sand mold casting, in order to realize sand molding, mold taking, pouring riser setting and sand core installation, the
Based on the national standard GB / T 9441-2009 metallographic examination of nodular cast iron, the following four parameters are
The pouring position usually refers to the position of the axle housing in the mold when pouring. The pouring position
In order to avoid too many times of Nitrocarburizing on different parts of lzqt600-3 ductile iron profile, the difficulty of
For cast steel, the main raw materials include scrap steel, ferrosilicon, manganese iron and aluminum alloy deoxidizer, and the main
During the production of lzqt600-3 ductile iron profile, due to its inherent process characteristics, the molten iron after spheroidizing treatment
(1) Scrap steel is the main raw material for casting smelting. Two samples are randomly selected from each batch for
Air tightness test, also known as sealing test, is an important indicator to judge whether there is internal defect in
The structural types of axle housing can be roughly divided into three types: open type, integral type and combined type.
In order to verify the feasibility of casting process, the sample of open axle housing was trial produced according to
The structural design of the axle housing can be roughly divided into the following aspects: the functional design of the
After adding riser and chill to the gating system, mesh division, casting parameters setting and pouring process simulation calculation are
Taking the tractor split axle housing as the research object, the paper firstly analyzes the process of the overall structure
The cold iron is directly attached to the area where the riser is not suitable. Because of the chilling effect
At present, most companies use sodium silicate sand mold casting and V-method casting process for production. In view of the
The ratio of the volume of the axle housing divided by the heat transfer surface area is called the solidification
As the key part of tractor, the main research contents are as follows: firstly, analyze the process of axle housing