Decarburization defect of quenched and tempered steel connecting rod during heat treatment
Decarburization refers to the phenomenon that CO2, H2O, O2, H2 and other gases in the heating medium interact with the […]
Decarburization refers to the phenomenon that CO2, H2O, O2, H2 and other gases in the heating medium interact with the […]
The new aluminum alloy ADC12-0.25ti containing titanium for automobile parts is taken as the research object. The chemical composition of
In the forming experiment, the large aluminum hub is taken as the forming object, with a diameter of 660mm and
In the situation of fierce market competition, under the premise of ensuring product quality, energy saving and consumption reduction is
The riser system in casting process design is generally designed based on experience and relevant databases. Sometimes the designed riser
Lost foam casting originated in the United States. In 1956, American H.F.Shiroyer used EPS foam as wax mold material for
No matter whether quenching + high temperature tempering or energy-saving waste heat quenching + high temperature tempering are used, the
30CrNiMo steel has been widely used in mining machinery due to its high hardenability, good comprehensive mechanical properties and excellent
ADC12-0.25ti aluminum alloy samples for automotive castings were prepared at different pouring temperatures. The microstructure, fluidity and hot cracking resistance
The system model of the composite squeeze casting forming system established provides the basis for the production logistics simulation of
The characteristics of compound squeeze casting die for large parts are as follows: only one cavity is set in one
Direct squeeze casting technology has a short pressure transmission distance because the pressure directly acts on the surface of liquid
The metallographic microstructure of the finished automobile connecting rod shall be uniform fine grain structure, and no sheet ferrite is
Additive manufacturing technology includes computer-aided design technology, material processing and forming technology. At the same time, digital model files need
(1) Prevent sand sticking of castings. After the coating penetrates into the surface of the sand mold (core), fill the
(1) Type of alloy used Theoretically, any metal that can be used for casting can be used for lost foam
In the past, the engine connecting rod was made of medium carbon steel or medium carbon alloy steel after quenching
ZL116 aluminum alloy has excellent casting performance, low hot cracking tendency, high air tightness, good mechanical properties, corrosion resistance and
Effect of chemical composition on mechanical properties Although the steel of the same brand will appear in production, some chemical
The production methods of engine connecting rods in China include traditional forging, casting and powder metallurgy, and the research and
In the process of industrial manufacturing, investment casting can play an important role and can be used to make parts
The lost foam casting process eliminates the complex processes such as core making, core baking, mold drawing, mold repair and
Intelligent manufacturing and green manufacturing are the development direction of China’s manufacturing industry. As the foundation of machinery manufacturing industry,
The process parameters of forging and quenching have a great influence on its strengthening effect. The main process parameters include:
The automobile connecting rod is made of fiber reinforced resin. After the fiber reinforced resin is adopted, its strength, stiffness
Cylinder head is one of the key components in engine parts. When a cylinder head product model is transformed into
Casting coating is a commonly used auxiliary material in casting production. It is a physical suspension dispersion system in colloidal
Lost foam casting is also called dry sand or negative pressure full mold casting, and its casting principle is shown
Lost foam casting Name: 105 type cable head; Material: ZG310-570; Geometric dimension: 620 mm × 290 mm × 210 mm;
Some manufacturers use high-strength titanium alloy to cast connecting rods, which are light in weight and insensitive to stress concentration.