Effect of carburizing defect on the composition of gold in lost foam Casting
According to the experimental results of the first two sections, the carburization defects will lead to the excessive chemical composition
According to the experimental results of the first two sections, the carburization defects will lead to the excessive chemical composition
The properties of tensile samples were tested by a universal testing machine controlled by microcomputer, and the tensile strength and
Six groups of samples were taken when analyzing surface carburization, and the location of the test point was changed to
In this test, 6 test pieces were poured in the same ladle of molten steel. The chemical composition of molten
By using ProCAST numerical simulation software to study the lost foam casting process of the representative steel and steel bearing
In order to study the carburization defects of steel casting for bridge support, four sampling locations are selected, namely, near
The filling process of lost foam casting is the replacement process of metal liquid and foam pattern. Because the pouring
Using the process plan after the second optimization, the small batch production verification of steel and steel bearing was carried
In order to study the impact resistance of steel castings at different temperatures, three temperature detection conditions, namely normal temperature,
When setting simulation parameters in ProCAST preprocessing section, the following aspects need to be adjusted: (1) The material of cold
In the process of heating and cooling, there will be group increase transformation of steel, which is the fundamental reason
The simulation results show that the safety height of riser is 11.15cm, which is 8.15cm higher than the minimum safety
Mechanical properties refer to the mechanical characteristics of materials under different environments when they bear various external loads (tensile, compression,
It can be seen from Fig. 1 that when the pouring temperature changes from high to low, the safe height
The object of this research is steel steel steel bearings in bridge bearings. The production process is produced according to
The safety height of riser feeding is taken as the evaluation index in the orthogonal test. The measurement method of
(a) Direct attack spectrometer The main instrument used for chemical composition detection is the direct attack spectrometer (q4-130) in Brooke,
The process parameters of lost foam casting have significant influence on the mechanical properties and the formation of carburizing defects.
The carburizing defects of steel castings can be divided into surface carburization, volume carburization and local carburization. Surface carburizing: during
The simulation parameters of vertical pouring scheme are consistent with those of horizontal pouring scheme, and other material configuration parameters
Lost Foam Casting (LFC) has been recognized by the foundry industry for its unique technological advantages. Many developed countries have
The steel and steel bearing trial produced by horizontal casting scheme is shown in Fig. 1. The overall appearance quality
The 3D drawing of horizontal pouring scheme is imported into ProCAST software. Firstly, the virtual sandbox is set up, and
The main functions of lost foam casting with negative pressure casting are as follows: (1) Compact the dry sand to
After entering the 21st century, a large number of domestic researchers still solved the problem of carbon enhancement. According to
Pouring temperature is a key factor affecting the quality of EPC Castings. If the pouring temperature is too high, the
Mechanism of carburization defects The mechanism of carburizing defect is the diffusion of carbon into soft moving molten steel and
Coating is an important part of lost foam casting process and one of the key factors affecting the filling of
China is also one of the earliest countries in the field of lost foam casting Technology Research (1965), which has
The advantages of EPC are dry sand molding, no binder is needed, the recovery rate of dry sand is high,