Quenched and tempered steel connecting rod
Structural steel after quenching and high temperature tempering has good comprehensive mechanical properties, high strength, good plasticity and toughness. The […]
Structural steel after quenching and high temperature tempering has good comprehensive mechanical properties, high strength, good plasticity and toughness. The […]
In addition to ductile iron and gray iron, vermicular iron and white iron are commonly used as cast iron alloys.
By imitating the surface characteristics of wear-resistant organisms, the bionic non smooth surface morphologies of point, strip and mesh are
(1) A forming method of composite squeeze casting for large parts was proposed. According to this method, a composite squeeze
The cylinder block is the framework of the automobile engine, with thin wall and complex structure. In the casting production,
When nodular cast iron is cast, the amount of nodularizing agent will directly affect the graphite morphology in cast iron,
The existence of flake graphite in the middle layer of gray cast iron seriously affects the improvement of its properties.
Connecting rod is one of the important components in the engine. Its quality directly affects the safe use and driving
Compared with the traditional squeeze casting die, the key problems to be solved in the composite squeeze casting die for
Connecting rod is an important part of mechanical transmission. It is necessary to use connecting rod to change the direction
The solid-state graphitization process of cast iron is essentially a process of transformation from metastable cementite to stable graphite. Graphitization
Fatigue wear failure of gray cast iron is a phenomenon that metal is removed from the contact area under the
The forming method and equipment of composite squeeze casting are studied theoretically and experimentally. The main research contents and conclusions
According to the design theory of production system, the structure of compound squeeze casting forming system is composed of logistics
The composite squeeze casting method and a composite squeeze casting forming system suitable for the squeeze casting of large parts
Mold is an important part of the forming system of composite squeeze casting for large parts. Composite squeeze casting is
Since the 1990s, researchers have carried out a lot of research on the surface modification of gray cast iron, among
The results show that the laser surface biomimetic strengthening technology can effectively improve the fatigue wear resistance of gray cast
Sand casting parts are a versatile and widely used manufacturing process with applications across numerous industries due to its ability
Laser surface strengthening technology is widely used because martensite, austenite, carbide and other strengthening phases occur in the machining area.
Composite squeeze casting is a complex forming method suitable for large parts. Because of its difficult process, high functional requirements
Forming method of composite squeeze casting for large castings, design and manufacture composite squeeze casting forming equipment and peripheral devices,
In order to make gray cast iron more widely used, the graphite morphology in gray cast iron must be strictly
According to the body surface characteristics of wear-resistant organisms, hard elements on such non smooth surfaces are often distributed in
G10mnmov6-3 low alloy cast steel cable clamp is heat treated by quenching + tempering. The heat treatment process is shown
The macroscopic fatigue defects of rolling fatigue wear are mainly formed by the propagation of fatigue microcracks. Fatigue micro cracks
According to the weight loss data of cast liner wear in the table, the relative wear coefficient of high chromium
20 ~ 60t medium frequency electric furnace is adopted for smelting, and the tapping temperature is controlled at 1580 ~
The ball mill has been running for six months under full load and full working conditions. As shown in the
Element C in g10mnmov6-3 low alloy cast steel cable clamp shall be controlled within 0.08% ~ 0.10%. Si can strengthen