Application of ductile iron gating system in prevention and control of surface slag inclusion defects
The whole process from molten iron smelting to casting completion is a complex and irreversible process. In the process of […]
The whole process from molten iron smelting to casting completion is a complex and irreversible process. In the process of […]
① According to the ratio of cross-sectional area, it is divided into closed gating system and open gating system. The
The main defect of the inlet cylinder casting in the NDT of VT, MT and Pt is that there are
(1) The surface quality and defects of the air inlet cylinder are mainly inspected by visual inspection (VT), magnetic particle
① The main function of the sprue is to guide molten iron into the runner or runner. According to the
According to the analysis of the casting structure and key casting technology difficulties of the intake cylinder, this paper mainly
The molten iron enters the mold filling process through the gating system, which can be seen as a liquid with
Before 2013, the company’s production performance of gas turbine castings was dominated by only a few small and medium-sized steel
The main characteristics of the magnetic traces of linear defects detected by MT are mainly linear aggregated magnetic traces with
Foreign technology status: Hangzhou Steam Turbine Casting and Forging Co., Ltd. pointed out in the patent technical background of “a
The main features of magnetic traces of point defects detected by MT. The magnetic traces are scattered and isolated small
According to the data reported by China Foundry Association at the industry annual meeting in recent years, the total amount
The inlet cylinder is one of the typical high difficulty ductile iron castings. Its solidification characteristics are closely related to
Ductile iron is an important kind of strong and tough cast iron, which has been fully used in heavy and
The inlet cylinder casting is composed of flange, brace, volute and other parts of cross connection. In the study, the
Since 2002, with the adjustment of national energy policy and the increase of West to east gas transmission project and
Shrinkage cavity and shrinkage porosity are common internal casting defects in heavy position of ductile iron castings. The shrinkage cavity
Heavy duty gas turbine (HGT) is a large-scale energy and power equipment which integrates many high technologies such as unit
In terms of gas turbine market prospect analysis, relying on the background of our company as the power main engine
Nodular cast iron intake cylinder is one of the important parts in the front end of heavy duty gas turbine
The important characteristics of five development stages of foreign gas turbine are summarized as follows: Birth stage (1939-1950): heavy duty
The section shape of gating system runner mainly refers to the section shape of ingate and cross runner. The cross-section
In the early 1940s, gas turbine began to set foot in the field of energy equipment in the power generation
The research of gating system parameters design is to analyze the statistical law of pouring process parameters, mainly including flow
Compared with the developed countries in the west, the foundation of engine manufacturing in China is weak, and the continuity
30 casting samples of cylinder block were selected. The pouring information was counted, including the casting mass (unit: kg), pouring
The results show that the size of the cylinder block is qualified and there is no obvious defect on the
The technological principle of pouring system for cylinder body iron castings is: conveying liquid metal to the inside of the