Current situation of equipment and wear-resistant casting in sandstone industry
Sandstone industry directly or indirectly affects the development of some industries, such as construction industry and cement industry. With the
Sandstone industry directly or indirectly affects the development of some industries, such as construction industry and cement industry. With the
Titanium and titanium alloy have many excellent properties, such as low density, high specific strength, corrosion resistance, small linear expansion
During the continuous cooling process after solidification, if the solid shrinkage of the casting is obstructed by Yin, the internal
1. Application abroad Volkswagen is the first automobile company to apply magnesium alloy on a large scale in automobiles. As
The research shows that about 75% of the fuel consumption is related to the vehicle mass. Reducing the vehicle mass
Shrinkage is the physical nature of the alloy. Under normal pouring temperature, the shrinkage volume of the alloy with fixed
Since the 12th Five Year Plan, China’s foundry industry has continued to develop steadily, but its growth rate has slowed
Formation of casting shrinkage cavity and shrinkage cavity during the solidification process of liquid metal in the mold, due to
The progress of machine tool casting in China in the past 30 years can be seen in China International Casting
1.Shrinkage in the process of solidification and cooling, the reduction of volume and size is called shrinkage. Shrinkage is the
With the development of China’s economy, automobile, energy, ship, aviation, railway and other fields which are closely related to the
1 Rapid investment casting Investment casting, also known as “lost wax casting”, has a long history in China. It is
Pure metals are rarely used in casting production, and various alloys are generally used. In addition to the mechanical properties,
The test results show that the microstructure of the high chromium cast steel is: tempered martensite + eutectic carbide +
1 The core casting equipment technology has been stagnated for a long time in China (1) The performance of the
The shape and size of core head have a great influence on the processability and stability of core in mold
Attention shall be paid to the following items when purchasing casting coating: (1) Different materials of castings correspond to different
High temperature alloy precision casting is widely used in advanced weapon equipment, such as turbine case of aircraft engine, interstage
From the air pollution prevention and control law issued by the State Council and the Ministry of environmental protection, we
In order to draw the casting process diagram, the following process parameters must be selected after the casting scheme is
In recent years, although nodular iron castings, vermicular iron castings and various light alloy castings have been developed rapidly, but
The key technical indexes of casting coating have great influence on the quality of casting, as follows. Influencing factors of
With the rapid development of aviation manufacturing industry in recent years, large-scale precision titanium alloy castings are more and more
In recent years, the development of nodular cast iron is very fast in our country. The proportion of nodular cast
The choice of parting surface is also one of the key factors for the casting process. If the casting is
In many occasions, some people often mention the problem of trace elements in cast iron, which is also the concern
Generally, for a qualified casting coating product, in order to ensure the normal realization of the function of the casting
As a commercial metal structure material, magnesium alloy has the advantages of high specific strength, good casting formability, superior damping,
The production practice of iron mold sand covered casting pump valve castings shows that the iron mold sand covered casting