Study on the influence Mechanism of characteristic correlation process parameters in Sand Mold casting
The setting of sand casting process parameters is related to the characteristics of casting process design, such as casting dimension
The setting of sand casting process parameters is related to the characteristics of casting process design, such as casting dimension
Among all the casting processes, sand casting is the most commonly used casting method. The molding materials of casting are
Sand casting is widely used in the forming of iron castings, non-ferroalloy castings and small steel castings, and occupies an
At present, there are still many problems in China’s manufacturing industry, such as low-carbon manufacturing, energy saving, insufficient investment, low
The products of traditional manufacturing industry are widely used in various industries, which produce a lot of economic and social
In order to ensure the surface quality of the casting, according to the characteristics of large wall thickness, small volume,
As a special casting method, centrifugal casting has the following advantages compared with traditional sand casting: (1) Hollow cylindrical and
With the development of computer hardware and simulation software and the maturity of various finite element software, the application of
The design takes the tractor split axle housing as the research object. The axle housing is made of zg40mn low
When the molten metal is poured into the mold, the volume shrinkage will occur during cooling and solidification. This shrinkage
The numerical simulation of temperature field is the basis of ProCAST software simulation, and also the core module. Through the
In the filling process, the flow of molten metal will have a great impact on the quality of the axle
ProCAST casting computer simulation process: firstly, Creo software was used to establish the three-dimensional numerical model of the casting system
The gating system is the channel to guide liquid metal into the mold cavity in sand mold. Its structure is
Numerical simulation is a method that uses the correspondence between different things to verify measures. Numerical simulation is irreversible. Casting
Casting process parameters mainly include dimensional tolerance, linear shrinkage, draft angle and other aspects. The determination of these process parameters
Generally speaking, the higher the pouring temperature is, the better the fluidity of alloy liquid is, and the more favorable
For sand mold casting, in order to realize sand molding, mold taking, pouring riser setting and sand core installation, the
The pouring position usually refers to the position of the axle housing in the mold when pouring. The pouring position
For cast steel, the main raw materials include scrap steel, ferrosilicon, manganese iron and aluminum alloy deoxidizer, and the main
(1) Scrap steel is the main raw material for casting smelting. Two samples are randomly selected from each batch for
Air tightness test, also known as sealing test, is an important indicator to judge whether there is internal defect in
The structural types of axle housing can be roughly divided into three types: open type, integral type and combined type.
In order to verify the feasibility of casting process, the sample of open axle housing was trial produced according to
After adding riser and chill to the gating system, mesh division, casting parameters setting and pouring process simulation calculation are
Taking the tractor split axle housing as the research object, the paper firstly analyzes the process of the overall structure
The cold iron is directly attached to the area where the riser is not suitable. Because of the chilling effect
The ratio of the volume of the axle housing divided by the heat transfer surface area is called the solidification
As the key part of tractor, the main research contents are as follows: firstly, analyze the process of axle housing
Shrinkage cavity is a common casting defect, which is essentially a volume defect. According to the causes, it can be