High temperature life of aero-engine castings due to thermomechanical fatigue
Thermomechanical fatigue is indispensable for evaluating the high temperature life of aero-engine components and is one of the key performance
Thermomechanical fatigue is indispensable for evaluating the high temperature life of aero-engine components and is one of the key performance
Ti Al alloy has the advantages of high specific strength, specific rigidity, good high temperature oxidation resistance and creep resistance,
1. Selection of parting surface and pouring position of casting According to the structural characteristics of the castings, the bottom
Based on the fact that squeeze casting can form complex thick wall castings with dense internal structure and solution heat
Semi solid processing is a new technology with rapid development at present. Due to the high quality characteristics of squeeze
In general, as long as the process and tooling are set reasonably, the extrusion casting can be solution treated, but
1.Determination of pouring mode According to the current manufacturers of large-scale normal roll, due to the limitation of equipment, operation
In recent years, the development of squeeze casting technology is still inseparable from the theme of improving product quality and
Although the amount of magnesium used in automobile industry is increasing, its application in automobile is still limited. At present,
Beijing Baimu aviation materials Hi Tech Co., Ltd. is a specialized manufacturing platform for titanium alloy casting materials and process
1. Production process The 693 brake caliper and 812 brake caliper of ZHY casting are produced in the same line,
Before molding, assemble the core box according to the requirements, pay attention to the assembly sequence and the positioning of
In the 21st century, China’s squeeze casting technology will develop steadily and rapidly. Mainly reflected in the squeeze casting theory
Subcutaneous porosity is a common casting defect of nodular iron castings. The moisture in molding sand, resin in sand core,
1.Current situation The network manufacturing mode of foundry enterprises refers to a new mode that foundry enterprises adopt information technology
In view of the change of exhaust temperature of automobiles, the materials used in the exhaust manifolds of automobiles are
Due to the improvement of casting quality, casting precision, casting cost and casting automation, the future casting industry will develop
Squeeze casting technology has been used in the production of pneumatic instruments for many years. It is mainly used for
The common characteristics of special casting are: the casting size is accurate, the surface roughness value is low, closer to
Generally speaking, precision casting of automobile castings mainly refers to EPC and investment casting technology. With the development of automobile
1.Current situation Single crystal superalloy is the most important blade material of advanced gas turbine engine. China has made remarkable
With the increasing requirements of energy saving, environmental protection and reducing the cost of components, large-scale structural casting of aluminum
1.Application in automobile and motorcycle casting As one of the main directions of piston blank production, squeeze casting has produced
Among all kinds of casting methods, sand casting is the most common one. This is because it has many advantages:
Advantages of 3D printing technology in sand casting The emergence of 3D printing technology has certain advantages in additive manufacturing.
1.Current situation Large castings refer to large-scale casting products in major technical equipment, with high performance requirements, mainly steel castings.
China has been the world’s largest casting production for 16 consecutive years. In 2015, the total output of all kinds
In order to meet the requirements of lightweight and integration of components, a large number of large-scale complex thin-walled aluminum
Vacuum die casting is an advanced die casting technology, which can eliminate or reduce the defects such as air entrainment
On the whole, the academic research in the field of foundry in China is not backward, and many of the