1 Advantages and limitations of the investment casting process 1.1 Pros 1) The dimensional accuracy of investment castings is high
1 Advantages and limitations of the investment casting process 1.1 Pros 1) The dimensional accuracy of investment castings is high
1 Preamble The thickness of the middle partition of the double-channel vortex shell is 2mm, and the cold insulation defect
The bedside box is an important part of ordinary machine tools, mainly used for all kinds of machine tools to
0 Introduction Casting coating is one of the indispensable and important raw and auxiliary materials in the casting process, which
1 Product introduction and technical requirements At present, China’s new urbanization process has entered a new stage of high-quality development,
1 Technical Requirements The appearance of the split 9AT differential housing is shown in Figure 1, the design weight of
1 Material of cold iron The commonly used cold iron materials in our company include,1) The material of cast iron
1 Introduction In recent years, with the continuous improvement of environmental requirements, our company has changed the original cupola and
Automobile lightweight is one of the important measures to achieve energy conservation and emission reduction The development of new technologies
0 Introduction In recent years, under the demand for energy conservation, emission reduction and environmental protection, the R&D focus of
0 Introduction In the production process of complex castings, due to many production parameters and complex production environment, various defects
1 Introduction A twin-cylinder cylinder head is a twin-cylinder 250 displacement aluminum alloy twin-cylinder head produced by our company, made
As a basic casting process method in the foundry industry, sand casting is widely used in the manufacturing industry because
1 Structural characteristics of castings Spiral series products are a series of small batches and multiple models, with many product
The quality of the finished camshaft casting is affected both by a combination of multiple casting process parameters and by
ZL101A aluminum alloy is a commonly used cast aluminum-silicon-magnesium alloy, which has good fluidity, small shrinkage, low hot cracking tendency,
1 Introduction When developing a new product fan “three impellers”, our company encountered internal shrinkage hole defects and dynamic balance
The ductile iron front cover is made of QT700-2 and is produced using a green sand process. Because the hardness
0 Introduction Automotive engine cylinder heads have a complex structure and are generally cast from cast iron or aluminum alloy
1 Causes and prevention of sand defects As defined in GB5611-2017 Casting Terminology, sand removal is a meaty defect. Fleshy
1 Survey analysis 1.1 Current situation and existing problems Through the investigation of our large-scale casting mold, taking a flywheel
With the continuous improvement of locomotive speed and carrying capacity, higher requirements are put forward for the steel castings of
The company produces a rod-shaped casting (shown in Figure 1) with contour dimensions of φ40 mm ×326 mm, made of
0 Introduction Automotive engine heads have complex structures and are typically cast from cast iron or aluminum alloys, as shown
As a basic casting process method in the casting industry, sand casting is widely used in the manufacturing industry because
1 Preface Lost foam casting (EPC for short), also known as negative compaction casting, has been invented by Americans since
In order to find out the influence of the forging blank on the performance of the finished product, we used
It can be seen from Fig. 1-2 that the inoculation of nodular cast iron can provide conditions for graphite nucleation,
The comparison of validation results of the three process schemes is shown in the table. Overall, Scheme III has certain
In order to eliminate the shrinkage cavity and porosity defects caused by solidification shrinkage of molten iron, take the relatively